Test Data of etching SiO2 with CHF3/CF4/O2 (using this recipe only for Fluorine etch of the underneath layer)

From UCSB Nanofab Wiki
Revision as of 07:03, 30 January 2019 by John d (talk | contribs) (moved SEM images to table, changed "File:" link --> Direct link to file)
Jump to navigation Jump to search
ICP#2: 0.5Pa, 50/500W, CHF3/CF4/O2=35/5/10sccm, time=210 sec
Date Sample# Etch Rate (nm/min) Etch Selectivity (SiO2/PR) Averaged Sidewall Angle (o) SEM Images
10/5/2018 SiO2#01 95.2 0.74 77.9
1/28/2019 I21902 92.1 0.77 [1]