Dry Etching Recipes
From UCSB Nanofab Wiki
Revision as of 04:11, 17 September 2019 by
Thibeault
(
talk
|
contribs
)
(
diff
)
← Older revision
|
Latest revision
(
diff
) |
Newer revision →
(
diff
)
Jump to navigation
Jump to search
R
= Recipe is available. Clicking this link will take you to the recipe.
A
= Material is available for use, but no recipes are provided.
Dry Etching Recipes
RIE Etching
ICP Etching
Oxygen Plasma Systems
Other Dry Etchers
Material
RIE 1
(Retired)
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
DSEIII
(PlasmaTherm)
SLR Fluorine ICP (PlasmaTherm)
ICP Etch 1
(Panasonic 1)
ICP Etch 2
(Panasonic 2)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
Plasma Clean (YES EcoClean)
UV Ozone Reactor
Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Ag
Al
A
R1
R1
Au
A
Cr
A
R1
A
Cu
Ge
A
Mo
Ni
R1
Pt
R1
Ru
A
R1
Si
R1
R1
R1
Ta
Ti
R1
A
Al
2
O
3
R
Al
2
O
3 (Sapphire)
R1
A
AlGaAs
R1
R1
GaAs-AlGaAs Etch (Unaxis VLR)
AlGaN
R1
AlN
R1
CdZnTe
R1
GaAs
R1
R1
R1
GaAs-AlGaAs Etch (Unaxis VLR)
GaN
R1
R1
R1
GaSb
A
GaSb Etch Unaxis VLR)
HfO
2
InGaAlAs
InP-InGaAsP-InGaAlAs Etching (RIE 2)
InP-InGaAs-InAlAs Etch (Unaxis VLR)
InGaAsP
InP-InGaAsP-InGaAlAs Etching (RIE 2)
InP-InGaAs-InAlAs Etch (Unaxis VLR)
InP
InP-InGaAsP-InGaAlAs Etching (RIE 2)
A
A
InP-InGaAs-InAlAs Etch (Unaxis VLR)
ITO
R1
Photoresist
& ARC
A
R
R
R
A
A
SiC
R1
A
SiN
SiN
x
Etching (RIE 3)
R1
R1
A
SiO
2
SiO
2
Etching (RIE 3)
A
R1
R1
R1
SiOxNy
A
A
Ta
2
O
5
A
TiN
TiO
2
W-TiW
R1
A
ZnO
2
ZnS
R1
ZnSe
R1
ZrO
2
Material
RIE 1
(Retired)
RIE 2
(MRC)
RIE 3
(MRC)
RIE 5
(PlasmaTherm)
DSEIII
(PlasmaTherm)
SLR Fluorine ICP (PlasmaTherm)
ICP Etch 1
(Panasonic E626I)
ICP Etch 2
(Panasonic E640)
ICP-Etch
(Unaxis VLR)
Ashers
(Technics PEII)
Plasma Clean
(Gasonics 2000)
Plasma Clean (YES EcoClean)
UV Ozone Reactor
Plasma Activation
(EVG 810)
XeF2 Etch
(Xetch)
Vapor HF Etch
(uETCH)
CAIBE
(Oxford)
Category
:
Processing
Navigation menu
Personal tools
Create account
Log in
Namespaces
Page
Discussion
English
Views
Read
View source
View history
More
Search
InvisibleMenu
QuickLinks
Lab Rules
Common Questions/FAQ
Staff List
Equipment Signup
Chemicals + MSDS
Protofab
Equipment
Full Tool List
Lithography
Vacuum Deposition
Dry Etch
Wet Processing
Thermal Processing
Packaging
Metrology & Test
Recipes and Data
Lithography
Vacuum Deposition
Dry Etching
Wet Etching
Thermal Processing
Packaging Tools
Data + Info
Process Control Data
Tutorials
Calculators/Utilities
NanoFab Info
Research + Pubs
Tech Talks
Tools
What links here
Related changes
Special pages
Printable version
Permanent link
Page information