| Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments |
| Aluminum | Al | 2.70 | 1.08 | ||
| Antimony | Sb | 2.70 | 0.768 | ||
| Arsenic | As | 5.73 | 0.996 | ||
| Beryllium | Be | 1.85 | 0.543 | ||
| |||||||||||||||||||||
Materials Table
| |||||
|---|---|---|---|---|---|
| Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments |
| Aluminum | Al | 2.70 | 1.08 | ||
| Antimony | Sb | 2.70 | 0.768 | ||
| Arsenic | As | 5.73 | 0.996 | ||
| Beryllium | Be | 1.85 | 0.543 | ||