Thermal Evaporation Recipes
Back to Vacuum Deposition Recipes.
Thermal Evap 1
Materials Table (Thermal Evaporator 1)
Thermal Evap 2 (Solder)
Materials Table
| |||||
|---|---|---|---|---|---|
| Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments |
| Aluminum | Al | 2.70 | 1.08 | ||
| Antimony | Sb | 6.620 | 0.768 | ||
| Arsenic | As | 5.73 | 0.996 | ||
| Beryllium | Be | 1.85 | 0.543 | ||
| Boron | B | 2.54 | 0.389 | ||
| Cadmium | Cd | 8.64 | 0.682 | ||
| Cadmium sulfide | CdS | 4.83 | 1.02 | ||