PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
- SiN Standard Recipe
- SiN Data April 2014
- SiN 1000A Thickness uniformity 2014
- Low Stress Si3N4 - Variable Stress Recipes
- Low Stress Si3N4 - Variable Stress Plot
- Dep.rate~11.21nm/min
- HFe.r.~87nm/min
- Stress~476MPa
- Index~1.936
SiO2 deposition (PECVD #1)
- SiO2 Standard Recipe
- SiO2 Data (Deposition rate, Refractive Index, Stress, HF etch rate)
- SiO2 Data April 2014
- SiO2 1000A Thickness uniformity 2014