- 20:45, 2 November 2023 John d talk contribs deleted page SSI Solaris 150 - Operating Procedure (Moved data to another page: content was: "'''Solaris (SSI) RTP Operating Instructions''' 1) On the main system press the green power on button. You will hear a loud click and hear air flowing. If you do not hear anything after pressing the green button, try rotating the EMO button and then press the green power on button again. 2) Press down on the door lever and gently pull out the wafer tray. Verify that a previou...", and the only contributor was "Lingg"...)