- 15:55, 22 August 2026 John d talk contribs uploaded File:2026 CSMANTECH Paper-2366 - Foong Fatt - Machine Matching Methodology for Single-shot Lab to Lab Dry Etch Process Transfer.pdf (Machine Matching Methodology for Single-shot Lab to Lab Dry Etch Process Transfer Fatt Foong, Brian Thibeault, Noah Dutra, Demis D. John, Vraj Mehalana, Chandan Ramakrishnaiah, Shivakumar Bhaskaran, Jacky Tseng, Shimin Huang, Michio Aruga, Weldom Xie, Bokai Ma, Jeongho Ha, John Tamelier, Fubo Rao Conference: CS MANTECH Year: 2026 Topics Process Transfer Compound Semiconductors GaAs Design of Experiments InP Dry Etch Nanofabrication Abstract Small start-up companies benefit significantly...)