User contributions for Biljana
Jump to navigation
Jump to search
22 April 2020
- 20:2420:24, 22 April 2020 diff hist +1 Wafer Coating Process Traveler →Unaxis deposition - 300nm SiN film @250°C Tag: Visual edit
- 20:2420:24, 22 April 2020 diff hist +28 Wafer Coating Process Traveler →Unaxis deposition - 300nm SiN film @250°C Tag: Visual edit
- 18:3318:33, 22 April 2020 diff hist −13 ICP-PECVD (Unaxis VLR) →Documentation Tag: Visual edit
- 18:3318:33, 22 April 2020 diff hist −131 ICP-PECVD (Unaxis VLR) →Documentation Tag: Visual edit
- 18:3118:31, 22 April 2020 diff hist −988 Wafer Scanning process Traveler wafers scanning procedure current Tag: Visual edit
- 18:2918:29, 22 April 2020 diff hist −744 Wafer scanning process traveler →Scan before process calibration Tag: Visual edit
- 18:2518:25, 22 April 2020 diff hist −316 Wafer Scanning process Traveler →Wafers to Use Tag: Visual edit
- 18:2318:23, 22 April 2020 diff hist +454 Wafer scanning process traveler →Wafers to Use Tag: Visual edit
- 18:1418:14, 22 April 2020 diff hist −917 Wafer Coating Process Traveler →Unaxis deposition - SiO2 LDR film @250°C Tag: Visual edit
- 18:1018:10, 22 April 2020 diff hist +766 Wafer Coating Process Traveler →Unaxis deposition - SiO2 LDR film @250°C: correction on Unaxis recipes Tag: Visual edit
- 18:0218:02, 22 April 2020 diff hist −4 Wafer Coating Process Traveler →Unaxis deposition - SiO2 LDR film @250°C Tag: Visual edit
- 17:5717:57, 22 April 2020 diff hist +97 Wafer Coating Process Traveler →Unaxis deposition - SiO2 LDR film @250°C Tag: Visual edit
- 17:3717:37, 22 April 2020 diff hist +151 PECVD Recipes →Historical Particulate Data
- 17:3417:34, 22 April 2020 diff hist +1 PECVD Recipes →Historical Particulate Data
- 00:3600:36, 22 April 2020 diff hist +254 PECVD Recipes →Thin-Film Properties: corrections in Unaxis films Tag: Visual edit
- 00:3300:33, 22 April 2020 diff hist +237 PECVD Recipes →SiO2 250C Deposition (Unaxis VLR)
21 April 2020
- 20:3920:39, 21 April 2020 diff hist +123 ICP-PECVD (Unaxis VLR) →Documentation: added link Tag: Visual edit
- 20:2920:29, 21 April 2020 diff hist +105 PECVD Recipes →Thin-Film Properties: added one sentence Tag: Visual edit
- 20:2520:25, 21 April 2020 diff hist +116 Wafer Coating Process Traveler →Unaxis deposition - 300nm SiO2 LDR film @250°C Tag: Visual edit
- 19:2819:28, 21 April 2020 diff hist −3 PECVD Recipes →ICP-PECVD (Unaxis VLR)
- 19:2719:27, 21 April 2020 diff hist −4 PECVD Recipes →ICP-PECVD (Unaxis VLR)
- 19:2519:25, 21 April 2020 diff hist +32 PECVD Recipes →SiO2 250C Deposition (Unaxis VLR)
- 19:2419:24, 21 April 2020 diff hist +34 PECVD Recipes →SiN LS 250C Deposition (Unaxis VLR)
- 19:2219:22, 21 April 2020 diff hist −3 PECVD Recipes →ICP-PECVD (Unaxis VLR)
- 19:2219:22, 21 April 2020 diff hist −2 PECVD Recipes →SiN 250C deposition (Unaxis VLR)
- 19:2119:21, 21 April 2020 diff hist +37 PECVD Recipes →ICP-PECVD (Unaxis VLR)
- 19:1819:18, 21 April 2020 diff hist +1 PECVD Recipes →ICP-PECVD (Unaxis VLR)
- 19:1619:16, 21 April 2020 diff hist −268 PECVD Recipes →SiO2 250C Deposition (Unaxis VLR)
- 19:1419:14, 21 April 2020 diff hist +358 PECVD Recipes →ICP-PECVD (Unaxis VLR)
- 19:0519:05, 21 April 2020 diff hist −699 PECVD Recipes →ICP-PECVD (Unaxis VLR)
- 19:0319:03, 21 April 2020 diff hist +418 PECVD Recipes →ICP-PECVD (Unaxis VLR)
- 19:0219:02, 21 April 2020 diff hist +49 PECVD Recipes →SiN deposition (PECVD #1) Tag: Visual edit
- 18:5518:55, 21 April 2020 diff hist +120 PECVD Recipes →Standard Recipe
- 18:5418:54, 21 April 2020 diff hist +118 PECVD Recipes →Standard Recipe
- 18:5318:53, 21 April 2020 diff hist +112 PECVD Recipes →Standard Recipe
- 18:0218:02, 21 April 2020 diff hist −21 PECVD Recipes →Standard Recipe Tag: Visual edit
- 18:0018:00, 21 April 2020 diff hist +72 N STD SiO2 recipe Created page with "[https://wiki.nanotech.ucsb.edu/w/images/4/4f/Adv._PECVD2-STD_SiO2.xlsx]" current Tag: Visual edit
- 18:0018:00, 21 April 2020 diff hist +21 PECVD Recipes →SiO2 deposition (PECVD #2) Tag: Visual edit
- 17:5917:59, 21 April 2020 diff hist 0 File:Adv. PECVD2-STD SiO2.xlsx Biljana uploaded a new version of File:Adv. PECVD2-STD SiO2.xlsx current
- 17:5317:53, 21 April 2020 diff hist +1 PECVD Recipes →SiO2 deposition (PECVD #2)
- 17:4317:43, 21 April 2020 diff hist −93 PECVD Recipes →Standard Recipe
- 17:4317:43, 21 April 2020 diff hist −1 PECVD Recipes →Standard Recipe
- 17:4317:43, 21 April 2020 diff hist +2 PECVD Recipes →Standard Recipe
- 17:4217:42, 21 April 2020 diff hist +92 PECVD Recipes →Standard Recipe
- 17:3517:35, 21 April 2020 diff hist −91 PECVD Recipes →Standard Recipe
- 17:2917:29, 21 April 2020 diff hist +1 PECVD Recipes →Standard Recipe
- 17:2417:24, 21 April 2020 diff hist +69 PECVD Recipes →Standard Recipe Tag: Visual edit
- 17:1817:18, 21 April 2020 diff hist +4 PECVD Recipes →Standard Recipe Tag: Visual edit
- 17:1717:17, 21 April 2020 diff hist +17 PECVD Recipes →SiO2 deposition (PECVD #2) Tag: Visual edit
- 17:1617:16, 21 April 2020 diff hist −293 PECVD Recipes →Standard Recipe Tag: Visual edit