PECVD1 Recipes
Jump to navigation
Jump to search
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
SiO2 deposition (PECVD #1)
Other recipes (PECVD1)
- SiOxNy Recipe
- SiOxNy Data December 2014
- SiOxNy 3000A Thickness uniformity 2014
- LS SiN Recipe
- LS SiN Data December 2014
- LS SiN 3000A Thickness uniformity 2014
LS SiOxNy deposition (PECVD #1)
- SiOxNy Deposition Recipes - Varying N/O Ratio
- SiOxNy Stress/Index vs. O/N Ratio
- SiOxNy Recipe
- SiOxNy Data December 2014
- SiOxNy 3000A Thickness uniformity 2014