Dicing Saw Recipes (ADT 7100)

Cutting Parameters

Material Blade Type Spindle Speed Cut Speed
Blade Diam Flange Diam. Blade Exposure

Mounting/Unmounting Samples

The UV-Release Tape dispenser is most-often used for mounting sample for dicing.

The Tape Model installed is XYZXYZ. Data Sheet Here.

  • Procedure for mounting sample on UV-Release Tape
  • Full Release: 60 sec exposure
  • Partial Release for Shipping: 9 sec exposure

Surface Protection

Users most often use sacrificial photoresists to protect the surface from accumulating dicing dust. The static-buildup of dielectric films causes the dust to adhere strongly. Ensure that the PR thickness will adequately coat all your exposed topography (eg. use a ≥2µm thick PR for protecting 1.5-2.0µm tall etched features).

  1. Choose a photoresist of appropriate thickness, and spin-coat it & soft-bake it according to a standard recipe. Contact Alignment PR Recipes Stepper PR Recipes
  1. Perform your dicing
  2. Strip the PR in Acetone and ISO & N2 dry