Dicing Saw (ADT)
|
About
The ADT 7100 Dicing Saw is optimized for multi-angle dicing of thin, tight tolerance products up to 200 mm x 200 mm. It is currently setup for dicing up to 8” diameter wafers. Check the Dicing Saw Recipes page for the blades we currently stock.
Detailed Specifications
Operating Procedures
Recipe Recovery Procedure
Click on the Programming Workspace- Go to any recipe
- Click 'Recipe Import'

- Select 'd: [New Volume]' from 'Folder List'

- Open folder 'ADT'. Open Folder 'ADT-7100-8544150816'. Open folder 'db'. Open folder 'exports'
- Find you recipe in the box to the right and double click on it
- Verify group name is correct under 'Recipe Info'
- Click 'OK'
- Click 'Replace'
- Repeat for additional recipes
Recipes
- Packaging Recipes > Dicing Saw Recipes (ADT 7100)
Be sure to also see the methods for protecting your sample from dicing dust, and mounting/unmounting.