| Ovens - Overview of All Lab Ovens
|
|
|
|
|
|
See the full list of Thermal Processing tools here.
List of all lab ovens and capabilities/uses
| Oven Name + Link
|
Temperature Range/Capabilities
|
Programmable
|
Gases
|
Vacuum/Pressure Range
|
Typical Uses
|
SignupMonkey Reservation
|
| Oven 1
|
- Typically 95°C
- Passive Cooling
|
No, single temperature.
|
N/A
|
Atmosphere only
|
Drying glassware, general baking.
|
No. Users may change temperature.
|
| Oven 2
|
- Typically 100°C
- Passive Cooling
|
No, single temperature.
|
N/A
|
Atmosphere only
|
Drying glassware, general baking.
|
No. Users may change temperature.
|
| Oven 4: HeraTherm Oven
|
|
- Multi-step programmable
- Ramp Rate: only low/med/high (not numeric ramp rate).
- Gas flow not programmable
|
- N2 (manual flow setting)
- Atmosphere Purge
|
Atmosphere only
|
Bonding, BCB/Polymer curing.
|
No
Reserve with note in logbook.
|
| Blue-M Oven
|
- Max. temp. 350°C
- Passive Cooling
|
- Yes, fully programmable up to 2 stages.
- Gas flow not programmable
|
|
Atmosphere only
|
BCB/Polymer curing.
|
Sign Up For This Tool
|