Direct-Write Lithography Recipes
Jump to navigation
Jump to search
Back to Lithography Recipes.
Work In Progress This article is still under construction. It may contain factual errors. Content is subject to change. |
Photolithography Recipes for the Heidelberg MLA150 will go here.
Positive Resist (MLA150)
General notes: Hotplates used, filters, laser wavelengths, etc.
Resist | Spin Cond. | Bake | Thickness | Exposure Time | Focus Offset | PEB | Developer | Developer Time | Comments |
---|---|---|---|---|---|---|---|---|---|
SPR955CM0.9 | 3 krpm/30” | 95°C/60” | ~ 0.9 um | AZ300MIF |
Negative Resist (MLA150)
General notes: Hotplates used, filters, laser wavelengths, etc.
Resist | Spin Cond. | Bake | Thickness | Exposure Time | Focus Offset | PEB | Flood | Developer | Developer Time | Comments |
---|---|---|---|---|---|---|---|---|---|---|
AZ5214 | 6 krpm/30” | 95°C/60” | ~ 1.0 um | 60" | AZ300MIF | 60" |
|