Summary

Example of 16.32µm Deep Etched Silicon with 650nm thick UV6 Photoresist mask, 2µm Pitch. (Image Credit: Noah Dutra 2024-08). [STD_Bosch_Si example 8/26/24.]

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current20:44, 8 October 2024Thumbnail for version as of 20:44, 8 October 20241,280 × 1,026 (883 KB)Noahdutra (talk | contribs)STD_Bosch_Si example 8/26/24