Thermal Evap 2 (Solder)

From UCSB Nanofab Wiki
Revision as of 16:56, 13 March 2025 by Biljana (talk | contribs) (→Recipes)
Jump to navigation Jump to search
Thermal Evap 2 (Solder)
Location Bay 3
Tool Type Vacuum Deposition
Manufacturer Custom
Description ?

Primary Supervisor Michael Barreraz
(805) 893-4147
mikebarreraz@ece.ucsb.edu

Secondary Supervisor

Don Freeborn


Recipes Vacuum Deposition Recipes

SignupMonkey: Sign up for this tool


About

Thermal evaporator #2 is the designated "Solder" evaporator. The tool is used primarily for solder materials including Gold, Indium and Tin. See the Recipes section below for other materials used.

Use this tool for materials with low melting temperatures, or for materials that have a high risk of contamination in the e-beam evaporators.

Detailed Specifications

Wafers up to 12" can be mounted.

Documentation

Recipes

Plot