| Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments |
| Aluminum | Al | 2.70 | 1.08 | ||
| Antimony | Sb | 2.70 | 0.768 | ||
| Arsenic | As | 5.73 | 0.996 | ||
| Beryllium | Be | 1.85 | 0.543 | ||
| Boron | B | 2.54 | 0.389 | ||
| Cadmium | Cd | 8.64 | 0.682 | ||
| Cadmium sulfide | CdS | 4.83 | 1.02 | ||
| Cadmium telluride | CdTe | 5.85 | 0.980 | ||