PECVD Recipes
Jump to navigation
Jump to search
Back to Vacuum Deposition Recipes.
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
SiO2 deposition (PECVD #1)
PECVD 2 (Advanced Vacuum)
SiN deposition (PECVD #2)
SiO2 deposition (PECVD #2)
ICP-PECVD (Unaxis VLR)
SiN deposition (Unaxis VLR)
SiN (2% SiH4)
50° | 100° | 250° |
---|---|---|
SiN (2% SiH4 - No-Ar)
50° | 100° | 250° |
---|---|---|
SiN (2% SiH4 - No-Ar - Extra N2)
50° | 100° | 250° |
---|---|---|
SiN (100% SiH4 )
50° | 100° | 250° | |
---|---|---|---|
SiO2 deposition (Unaxis VLR)
SiO2 (2% SiH4)
50° | 100° | 250° |
---|---|---|
SiO2 (2% SiH4 - No Ar)
50° | 100° | 250° |
---|---|---|
SiO2 (100% SiH4 HDR)
50° | 100° | 250° |
---|---|---|
SiO2 (100% SiH4 LDR)
50° | 100° | 250° |
---|---|---|