Difference between revisions of "Dicing Saw (ADT)"
Jump to navigation
Jump to search
(→Detailed Specifications: deleted old SOP, Lee's SOP only) |
(SOP rev) |
||
Line 19: | Line 19: | ||
==Detailed Specifications== | ==Detailed Specifications== | ||
− | * Maximum Wafer Size: 8" | + | *Maximum Wafer Size: 8" |
− | * Parts mounted to UV-release tape for cutting | + | *Parts mounted to UV-release tape for cutting |
− | * Automated cut maps at multiple angles (0° and 90° typical) | + | *Automated cut maps at multiple angles (0° and 90° typical) |
− | * ~few micron alignment to on-wafer features. | + | *~few micron alignment to on-wafer features. |
− | * Thermocarbon Resnoid dicing blades provided by staff | + | *Thermocarbon Resnoid dicing blades provided by staff |
==Operating Procedures== | ==Operating Procedures== | ||
− | *[https://wiki.nanotech.ucsb.edu/w/images/ | + | *[https://wiki.nanotech.ucsb.edu/w/images/1/11/ADT_SOP_Rev_E.pdf ADT Dicing Saw Standard Operating Procedure] |
*[[ADT 7100 - Recovering an Old Recipe (2019)|Recovering an Old Recipe]] | *[[ADT 7100 - Recovering an Old Recipe (2019)|Recovering an Old Recipe]] | ||
Revision as of 13:48, 21 March 2022
|
About
The ADT 7100 Dicing Saw is optimized for multi-angle dicing of thin, tight tolerance products up to 200 mm x 200 mm. It is currently setup for dicing up to 8” diameter wafers. Check the Dicing Saw Recipes page for the blades we currently stock.
An ADT WM-966 tape applicator & Ultron Systems UH104-8 UV lamp system is used to apply UV-release tape for securing die during dicing.
Contact the tool supervisor for blades and dicing frames for your group.
Detailed Specifications
- Maximum Wafer Size: 8"
- Parts mounted to UV-release tape for cutting
- Automated cut maps at multiple angles (0° and 90° typical)
- ~few micron alignment to on-wafer features.
- Thermocarbon Resnoid dicing blades provided by staff