Two Spin-Rinse Dryers are available, one for 4-inch wafers and one for 6-inch wafers.
 
 
Each has a dedicated cassette that can hold up to 25 wafers.
 
 
The tool is set up to rinse at ~1000 rpm while spraying DI water, and then Dry in nitrogen at ~2000 rpm. A "Dry Only" option is also available.
 
 
{{tool|{{PAGENAME}}
 
 
|picture=SpinRinse.jpg
 
|picture=SpinRinse.jpg
 
|type = Wet Processing
 
|type = Wet Processing
|super= Don Freeborn
+
|super= Michael Barreraz
  +
|super2= Don Freeborn
|location=Bay 7
+
|location=Bay 5
 
|description = ?
 
|description = ?
 
|manufacturer = SemiTool
 
|manufacturer = SemiTool
 
}}
 
}}
  +
 
Two Spin-Rinse Dryers are available, one for 4-inch wafers and one for 6-inch wafers.
  +
 
Each has a dedicated cassette that can hold up to 25 wafers.
  +
 
The tool is set up to rinse at ~1000 rpm while spraying DI water, and then Dry in nitrogen at ~2000 rpm. A "Dry Only" option is also available.

Latest revision as of 11:02, 30 August 2022

Spin Rinse Dryer (SemiTool)
SpinRinse.jpg
Location Bay 5
Tool Type Wet Processing
Manufacturer SemiTool
Description ?

Primary Supervisor Michael Barreraz
(805) 893-4147
mikebarreraz@ece.ucsb.edu

Secondary Supervisor

Don Freeborn


Recipes N/A


Two Spin-Rinse Dryers are available, one for 4-inch wafers and one for 6-inch wafers.

Each has a dedicated cassette that can hold up to 25 wafers.

The tool is set up to rinse at ~1000 rpm while spraying DI water, and then Dry in nitrogen at ~2000 rpm. A "Dry Only" option is also available.