Difference between revisions of "Surface Analysis (KLA/Tencor Surfscan)"
Jump to navigation
Jump to search
(→About) |
|||
Line 18: | Line 18: | ||
**''For detailed measurement info, it is highly recommended that you read the manual.'' |
**''For detailed measurement info, it is highly recommended that you read the manual.'' |
||
*[//wiki.nanotech.ucsb.edu/w/images/2/27/Surfscan-Surfscan_6200_info.pdf Surfscan Info] |
*[//wiki.nanotech.ucsb.edu/w/images/2/27/Surfscan-Surfscan_6200_info.pdf Surfscan Info] |
||
+ | * |
||
− | |||
=== Screenshots === |
=== Screenshots === |
||
[[File:UCSBTEST.png|left|thumb|'''UCSBTEST2''' for big size particles '''(1.6-28.0)um''']][[File:UCSBTEST2 for small particles.png|left|thumb|'''UCSBTEST2''' for small size particles '''(0.16-1.6)um''']] |
[[File:UCSBTEST.png|left|thumb|'''UCSBTEST2''' for big size particles '''(1.6-28.0)um''']][[File:UCSBTEST2 for small particles.png|left|thumb|'''UCSBTEST2''' for small size particles '''(0.16-1.6)um''']] |
Revision as of 15:18, 31 March 2020
|
About
This system uses a laser-based scattering method to count size and distribution of particles (or other scattering defects) on a flat wafer surface. It can scan wafers in size from 4 to 8 inches.
Documentation
- Standard Operating Procedure
- Operations Manual
- For detailed measurement info, it is highly recommended that you read the manual.
- Surfscan Info