Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments |
Aluminum | Al | 2.70 | 1.08 | ||
Antimony | Sb | 2.70 | 0.768 | ||
Arsenic | As | 5.73 | 0.996 | ||
Beryllium | Be | 1.85 | 0.543 | ||
Boron | B | 2.54 | 0.389 | ||
Cadmium | Cd | 8.64 | 0.682 | ||
Cadmium sulfide | CdS | 4.83 | 1.02 | ||
Cadmium telluride | CdTe | 5.85 | 0.980 | ||
Calcium fluoride | CaF2 | 3.18 | 0.775 | ||
Carbon (graphite) | C | 2.25 | 3.26 | ||
Chromium | Cr | 7.20 | 0.305 | ||
Cobalt | Co | 8.71 | 0.343 | ||
Copper | Cu | 8.93 | 0.437 | ||
Gallium | Ga | 5.93 | 0.593 | ||
Gallium Arsenide | GaAs | 5.31 | 1.59 |