Difference between revisions of "Thermal Evap 2 (Solder)"
Jump to navigation
Jump to search
Line 176: | Line 176: | ||
|11.3 |
|11.3 |
||
|1.13 |
|1.13 |
||
+ | | |
||
+ | | |
||
+ | |- |
||
+ | |Lead sulfide |
||
+ | |PbS |
||
+ | |7.50 |
||
+ | |0.566 |
||
+ | | |
||
+ | | |
||
+ | |- |
||
+ | |Lithium fluoride |
||
+ | |LiF |
||
+ | |2.64 |
||
+ | |0.774 |
||
+ | | |
||
+ | | |
||
+ | |- |
||
+ | |Magnesium |
||
+ | |Mg |
||
+ | |1.74 |
||
+ | |1.61 |
||
+ | | |
||
+ | | |
||
+ | |- |
||
+ | |Magnesium oxide |
||
+ | |MgO |
||
+ | |3.58 |
||
+ | |0.411 |
||
+ | | |
||
+ | | |
||
+ | |- |
||
+ | |Manganese |
||
+ | |Mn |
||
+ | |7.20 |
||
+ | |0.377 |
||
| |
| |
||
| |
| |
Revision as of 15:41, 28 August 2012
|
About
Materials Table
Materials Table
| |||||
---|---|---|---|---|---|
Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments |
Aluminum | Al | 2.70 | 1.08 | ||
Antimony | Sb | 2.70 | 0.768 | ||
Arsenic | As | 5.73 | 0.996 | ||
Beryllium | Be | 1.85 | 0.543 | ||
Boron | B | 2.54 | 0.389 | ||
Cadmium | Cd | 8.64 | 0.682 | ||
Cadmium sulfide | CdS | 4.83 | 1.02 | ||
Cadmium telluride | CdTe | 5.85 | 0.980 | ||
Calcium fluoride | CaF2 | 3.18 | 0.775 | ||
Carbon (graphite) | C | 2.25 | 3.26 | ||
Chromium | Cr | 7.20 | 0.305 | 155 | |
Cobalt | Co | 8.71 | 0.343 | ||
Copper | Cu | 8.93 | 0.437 | ||
Gallium | Ga | 5.93 | 0.593 | ||
Gallium Arsenide | GaAs | 5.31 | 1.59 | ||
Germanium | Ge | 5.35 | 0.516 | ||
Gold | Au | 19.30 | 0.381 | ||
Indium | In | 7.30 | 0.841 | 120 | |
Indium antimonide | InSb | 5.76 | 0.769 | ||
Iridium | Ir | 22.4 | 0.129 | ||
Iron | Fe | 7.86 | 0.349 | ||
Lead | Pb | 11.3 | 1.13 | ||
Lead sulfide | PbS | 7.50 | 0.566 | ||
Lithium fluoride | LiF | 2.64 | 0.774 | ||
Magnesium | Mg | 1.74 | 1.61 | ||
Magnesium oxide | MgO | 3.58 | 0.411 | ||
Manganese | Mn | 7.20 | 0.377 |