(Replaced content with "There are three standard recipes : STD SiO2, STD Nitride2, and STD LS Nitride2 at 300C. Instructions bellow explain how to run each of the recipes ( seasoning, deposition,...")
Tags: Replaced Visual edit
Line 9: Line 9:
 
==== Standard nitride deposition ====
 
==== Standard nitride deposition ====
  
=== STD LS Nitride2 at 300C ===
+
=== STD LS Nitride2 ===
  
 
==== Standard low stress nitride deposition ====
 
==== Standard low stress nitride deposition ====

Revision as of 16:43, 22 April 2020

There are three standard recipes : STD SiO2, STD Nitride2, and STD LS Nitride2 at 300C. Instructions bellow explain how to run each of the recipes ( seasoning, deposition, cleaning)

STD SiO2

Standard oxide deposition

STD Nitride2

Standard nitride deposition

STD LS Nitride2

Standard low stress nitride deposition