Wafer Scanning/Coating Process Traveler ( combined/less detailed)

From UCSB Nanofab Wiki
Revision as of 09:39, 20 April 2020 by Biljana (talk | contribs)
Jump to navigation Jump to search

WIP....

The wafers for process calibration are ordered from SVM (https://www.svmi.com/). These are: 4” Si wafers, P/Boron, <100>, 1-30 ohm-cm, 525 +/-25 microns, Polished/Etched, Particles: <=10 @ >=0.3 microns, and have low LPD count (LPD= light particle detection, LPD<100).

Scan before process calibration