=Materials Table=
==Materials Table==


{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
Line 215: Line 215:
|0.1
|0.1
|
|
|-
|}


=[[Thermal Evaporator 2]]=
=[[Thermal Evaporator 2]]=


== Materials Table ==
== In Deposition (Thermal Evaporator 2) ==
*[[media:Thermal evaporator 2 Sheet1.pdf|Indium evaporation Data]]

= Materials Table =


{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
Line 647: Line 644:
|
|
|
|
|-
|}

== In Deposition (Thermal Evaporator 2) ==
*[[media:Thermal evaporator 2-new Sheet1.pdf|Indium evaporation Data]]

Revision as of 00:00, 27 June 2018

Back to Vacuum Deposition Recipes.

Thermal Evaporator 1

Materials Table

Thermal Evaporator 2

Materials Table