Autostep 200 Troubleshooting and Recovery: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
No edit summary
Line 58: Line 58:
[[File:Autostep 200 Upper keyboard.png|frame|none]]
[[File:Autostep 200 Upper keyboard.png|frame|none]]


3) Open the lower cabinet and pull out the lower keyboard, quickly press '''“scroll lock”''' twice followed immediately by the '''“up arrow key”.'''
[[File:Lower keyboard.png|none|thumb]]
4) On the same lower keyboard, press “'''alt & x'''”.


5) Press “'''enter”'''.


6) In the lower cabinet, turn off '''the computer (#2)-(smart set)''' below the keyboard. Press the '''power''' button.
[[File:Computer-2 -smart set.png|none|thumb]]
7) Retrieve the keys on the key chain. – located in the lower cabinet in front of the computer.
8) Open the tall cabinet to the left.
[[File:Autostep Cabinet .png|none|thumb]]
9) Use the keys to open the locked '''main computer ( #1)- (kontron)'''. Black flip down module.  Turn off this computer.
[[File:Autostep main computer -1.png|left|thumb|191x191px]]
[[File:Autostep main computer switch.png|none|thumb|189x189px]]


10)          

3) Open the lower cabinet and pull out the lower keyboard, quickly press “scroll lock” twice followed immediately by the “up arrow key”.

Revision as of 16:15, 24 March 2020

WIP...

Troubleshooting

What to do in case of computer (monitor) freeze-up.  Please try these things in this order.

1)    Try CTRL C followed by A and Enter.  This will abort any command that may have hung up.

2)    For Reticle Robot Hang Up:  See step 25 of start-up procedure. 

What to do in case of unplanned power outage.

     1)  CR Staff will take care of the system in the morning.

What to do for alignment error.

1)   Verify that correct alignment key offset is being used

2)   If you have DFAS alignment marks, perform a MAP job to verify alignment.

What to do for focus resolution problems.

1)   Perform a focus (EXPO) job using the same type of wafer that you will use for your real job and use the optimal focus offset determined from this job.  You may need to look at both exposure time and focus.

2)   If you have been running the same process and now have issues, run SETUP from the : prompt, following the instructions on the GCA Regular Maintenance Sheet.

What to do in case of the stage limit going too far (red stage limit light will be lit inside the stepper chamber next to the joystick.

1)   Press the lit limit switch to release the stage.

Contacts to call if you cannot undo the problem. Do not call after 10 p.m. unless there is a real emergency (A deadline for a paper or conference is not a real emergency)

1)    Mike Silva : x 3918 x 219 Work

2)    Brian Thibeault : x 2268 Work

3)    Biljana Stamenic:x4002 Work

4)    3c technical.  (These guys know all about the stepper, they rebuilt it and service it under contract for us).   Ask for Matt or Adam.

         matt@3ctechnical.com
         www.3ctechnical.com
         480-963-4559 voice
         480.212.0932 fax

5)    Send e-mail to nanofab@ece.ucsb.edu and report the problem.

Restarting procedure

Power down:

1) Press “ctrl C & A” to abort any currently running process.

2) If the system is frozen skip to step 3

If not, press “ctrl & ] (right bracket) “ on the upper keyboard. (The main keyboard under the alignment screens)

Autostep 200 Upper keyboard.png

3) Open the lower cabinet and pull out the lower keyboard, quickly press “scroll lock” twice followed immediately by the “up arrow key”.

Lower keyboard.png

4) On the same lower keyboard, press “alt & x”.

5) Press “enter”.

6) In the lower cabinet, turn off the computer (#2)-(smart set) below the keyboard. Press the power button.

Computer-2 -smart set.png

7) Retrieve the keys on the key chain. – located in the lower cabinet in front of the computer. 8) Open the tall cabinet to the left.

Autostep Cabinet .png

9) Use the keys to open the locked main computer ( #1)- (kontron). Black flip down module.  Turn off this computer.

Autostep main computer -1.png
Autostep main computer switch.png

10)