Dry Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
(deleted Unaxis Etch column) |
(→Dry Etching Tools/Materials Table: Changed Si etch on FICP from R3 to R5) |
||
Line 226: | Line 226: | ||
| |
| |
||
|{{rl|ICP Etching Recipes|DSEIII_(PlasmaTherm/Deep_Silicon_Etcher)}} |
|{{rl|ICP Etching Recipes|DSEIII_(PlasmaTherm/Deep_Silicon_Etcher)}} |
||
|[[ICP Etching Recipes#Si Etching .28Fluorine ICP Etcher.29| |
|[[ICP Etching Recipes#Si Etching .28Fluorine ICP Etcher.29|R5]] |
||
| |
| |
||
| |
| |
Revision as of 17:15, 9 August 2024
Process Control Data
See above linked page for process control data (dep rate/stress etc. over time), for a selection of often-used dry etches
Dry Etching Tools/Materials Table
The Key/Legend for this table's A...R6
values is at the bottom of the page.
Process Ranking Table
Processes in the table above are ranked by their "Process Maturity Level" as follows:
Process Level | Description of Process Level Ranking | ||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|
A | Process Allowed and materials available but never done | ||||||||||
R1 | Process has been run at least once | ||||||||||
R2 | Process has been run and/or procedure is documented or/and data available | ||||||||||
R3 | Process has been run, procedure is documented, and data is available | ||||||||||
R4 | Process has a documented procedure with regular (≥4x per year) data or lookahead/in-situ control available | ||||||||||
R5 | Process has a documented procedure with regular (≥4x per year) data and lookahead/in-situ control available | ||||||||||
R6 | Process has a documented procedure, regular ( ≥4x per year) data, and control charts & limits available |