Surfscan SOP for 8inch wafers: Difference between revisions
Surfscan 8 inch |
(No difference)
|
Latest revision as of 23:00, 20 November 2024
Important Guidelines
● Wafer Thickness: Do not use wafers thicker than 1 mm.
● Always log off after completing your session.
● Log all scans and issues in the logbook after use.
Procedure
1. Login Instructions
● Access Code: fab (new password from 2025].
● If the keyboard isn’t functional, use the virtual keyboard on the monitor.
● Double-click the SCAN icon to launch the software.
2. Loading a Recipe
- Navigate to Recipe > Load (upper-left corner).
- Select one of the standard recipes for 8-inch wafers:
○ STD_UCSB_8INCH_G2 (1.6–28 µm).
○ STD_UCSB_8INCH_G4 (0.16–1.6 µm).
- Do not make any changes in the recipe.
- Click OK. The recipe name will appear at the top of the screen.
3. Customizing a Recipe
- Select Recipe > Save as and name the recipe (e.g., your name or company name).
- Select Recipe > View/Modify to adjust the following parameters:
○ Wafer diameter
○ Edge exclusion
○ Gain
○ Threshold
○ Indexer
- Under Bin Split, click Default Bin to apply changes.
- Save the updated recipe.
4. Loading Wafers
- Use the black cassette for 8-inch wafers.
- Load the wafers with the face up, and the major flat away from you.
- Place the cassette in the left indexer (specific for 8-inch wafers).
- Ensure the cassette is seated properly.
- On the monitor, select CASS (Cassette) and wait for the tool to detect the wafers.
5. Scanning Wafers
To Scan a Single Wafer:
● Select the desired wafer from the monitor.
● Click START (upper menu bar).
● Wait for the scan to finish and record the results.
To Scan Multiple Wafers:
● Select AUTO mode.
● Click START to begin scanning all wafers in the cassette.
6. After Scanning
- Once the scan is complete:
○ Press ENTER on the small laptop to save the scan as a photo.
○ Location: Desktop/Local Disk(C)/Users/Public/Public Documentation.
○ Photos can be accessed/downloaded via the Nanofab server.
○ Note: Full data-saving functionality will be available in January 2025.
- Click HOME, select RECIPE/Exit, and log off.
Reminders
● Always ensure the cassette is seated properly in the left indexer.
● Log off after completing your session.