Vacuum Deposition Recipes: Difference between revisions
Jump to navigation
Jump to search
(Updated EB4 Ti/Au/Cr/Ni to R6 & linked to Process Control data) |
|||
Line 3: | Line 3: | ||
===Deposition Tools/Materials Table=== |
===Deposition Tools/Materials Table=== |
||
''The Key/Legend for this table's <code> |
''The Key/Legend for this table's <code>R1...R6</code> values is at the [[Vacuum Deposition Recipes#Process Ranking Table|<u>bottom of the page</u>]].'' |
||
{| class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;" border="1" |
{| class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;" border="1" |
||
|- bgcolor="#d0e7ff" |
|- bgcolor="#d0e7ff" |
Revision as of 17:55, 5 March 2025
Process Control Data
See linked page for process control data (calibration data over time, such as dep. rate, refractive index, stress etc.) over time, for a selection of highly used tools/films.
Deposition Tools/Materials Table
The Key/Legend for this table's R1...R6
values is at the bottom of the page.
Process Ranking Table
Processes in the table above are ranked by their "Process Maturity Level" as follows:
Process Level | Description of Process Level Ranking | ||||||||||
A | Process Allowed and materials available but never done | ||||||||||
R1 | Process has been ran at least once | ||||||||||
R2 | Process has been ran and/or procedure is documented or/and data available | ||||||||||
R3 | Process has been ran, procedure is documented, and data is available | ||||||||||
R4 | Process has a documented procedure with regular (≥4x per year) data or lookahead/in-Situ control available | ||||||||||
R5 | Process has a documented procedure with regular (≥4x per year) data and lookahead/in-Situ control available | ||||||||||
R6 | Process has a documented procedure, regular ( ≥4x per year) data, and control charts/limits available |