Field Emission SEM 2 (JEOL IT800SHL): Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
mNo edit summary |
|||
(One intermediate revision by one other user not shown) | |||
Line 15: | Line 15: | ||
Identical to [https://wiki.nanofab.ucsb.edu/wiki/SEM_1_(JEOL_IT800SHL) SEM#1], but with EDAX module added. |
Identical to [https://wiki.nanofab.ucsb.edu/wiki/SEM_1_(JEOL_IT800SHL) SEM#1], but with EDAX module added. |
||
Please see the [https://wiki.nanofab.ucsb.edu/wiki/SEM_1_(JEOL_IT800SHL) SEM#1 page] for main tool details. |
'''Please see the [https://wiki.nanofab.ucsb.edu/wiki/SEM_1_(JEOL_IT800SHL) SEM#1 page] for main tool details & procedures.''' |
||
== |
==EDS Elemental Analysis== |
||
*EDS Operating Procedure |
|||
*[https://wiki.nanofab.ucsb.edu/w/images/3/3a/EDS_SOP.jpg EDS Operating Procedure] |
Latest revision as of 04:08, 1 March 2024
|
About
The JEOL IT800HSL Field Emission Scanning Electron Microscope is used for imaging a variety of samples made in the facility.
Identical to SEM#1, but with EDAX module added.
Please see the SEM#1 page for main tool details & procedures.