Surface Analysis (KLA/Tencor Surfscan): Difference between revisions
Jump to navigation
Jump to search
(27 intermediate revisions by the same user not shown) | |||
Line 25: | Line 25: | ||
*[https://wiki.nanofab.ucsb.edu/w/images/2/29/Wafer_Particle_Count-Process_Traveler.pdf Wafer Scanning Instructions] |
*[https://wiki.nanofab.ucsb.edu/w/images/2/29/Wafer_Particle_Count-Process_Traveler.pdf Wafer Scanning Instructions] |
||
**''This is the procedure Staff uses to calibrate particle counts on our deposition tools. |
**''This is the procedure Staff uses to calibrate particle counts on our deposition tools. After the scan is complete you need to press ENTER on a small laptop. The Data will be saved on: Desktop/Local Disk(C)/Users/Public/Public Documentation] The data will be saved as a photo. |
||
'' |
|||
Surfscan instructions [wafers different size, and pieces] |
* Surfscan instructions [wafers different size, and pieces]: |
||
⚫ | |||
*[https://wiki.nanofab.ucsb.edu/w/images/a/a2/SURFSCAN_6200_122123_for_8inch_wafers.pdf Surfscan 6200 8inch wafers Scanning 8inch wafers] |
|||
*[https://wiki.nanofab.ucsb.edu/w/images/1/1a/SURFSCAN_6200_122023_for_6inch_wafers.pdf Surfscan 6200 6inch wafers] * |
|||
*[https://wiki.nanofab.ucsb.edu/w/images/9/9f/SURFSCAN_6200_122123_for_4inch_wafers.pdf Surfscan 6200 4inch wafers] * |
|||
*[https://wiki.nanofab.ucsb.edu/w/images/a/a7/SURFSCAN_6200_122123_small_substrates.pdf Surfscan 6200 [Small samples, and 2inch and 3inch wafers]] * |
|||
⚫ | |||
*[https://drive.google.com/drive/folders/1A-EOaVv7BZ7LqBU-ootweDXzz8KXIF3s 6inch wafers] |
|||
*[https://drive.google.com/drive/folders/1EUoxJusqM7We6EMnK64aG08ijyCjwt3U 4inch wafers] |
|||
*[https://drive.google.com/drive/folders/1ypVvJM5PEay0fwscYaWHG53XlYlmpJUF All kind of small substrates] |
|||
**''You must water-mount your small sample or wafer(2inch or 3 inch) to a 4-inch wafer.'' |
**''You must water-mount your small sample or wafer(2inch or 3 inch) to a 4-inch wafer.'' |
||
*[[Wafer scanning process traveler|Wafer Particle Count - Process Traveler]] |
*[[Wafer scanning process traveler|Wafer Particle Count - Process Traveler]]- Very detailed instructions |
||
===Other Documentation=== |
===Other Documentation=== |
Latest revision as of 17:59, 3 October 2024
|
About
This system uses a laser-based scattering method to count size and distribution of particles (or other scattering defects) on a flat wafer surface.
It can scan wafers in size from 4 to 8 inches. Piece-parts are more difficult but can be scanned with a custom recipe.
4-inch wafers are the most standard size to measure.
For measuring very low particle counts accurately, purchase "low particle count" (LPC) wafers from a Silicon wafer vendor, and keep the wafers in the case and clean at all times until use.
Documentation
Operating Procedures
- Wafer Scanning Instructions
- This is the procedure Staff uses to calibrate particle counts on our deposition tools. After the scan is complete you need to press ENTER on a small laptop. The Data will be saved on: Desktop/Local Disk(C)/Users/Public/Public Documentation] The data will be saved as a photo.
- Surfscan instructions [wafers different size, and pieces]:
- 8inch wafers
- 6inch wafers
- 4inch wafers
- All kind of small substrates
- You must water-mount your small sample or wafer(2inch or 3 inch) to a 4-inch wafer.
- Wafer Particle Count - Process Traveler- Very detailed instructions
Other Documentation
- Operations Manual
- For detailed measurement info, it is highly recommended that you read the manual.
Examples
Gain 4: Small Particles
(0.160µm – 1.60µm) |
Gain 2: Large Particles
(1.60µm – 28.0µm) |
---|---|
Gain 4: Small Particles
(0.160µm – 1.60µm) |
Gain 2: Large Particles
(1.60µm – 28.0µm) |
---|---|