Vacuum Deposition Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
No edit summary |
Added some known R1 materials to Ebeam 1+4 |
||
| (4 intermediate revisions by 2 users not shown) | |||
| Line 126: | Line 126: | ||
|- |
|- |
||
!AuPd |
!AuPd |
||
|R1 |
|||
| |
| |
||
| |
| |
||
| |
|R1 |
||
| |
|||
| |
| |
||
| |
| |
||
| Line 177: | Line 177: | ||
|- |
|- |
||
!AuGe |
!AuGe |
||
|[[E-Beam Evaporation Recipes#E-Beam 1 .28Sharon.29| |
|[[E-Beam Evaporation Recipes#E-Beam 1 .28Sharon.29|R2]] |
||
| |
|||
| |
|||
| |
| |
||
|R1 |
|||
|R2 |
|||
| |
| |
||
| |
| |
||
| Line 315: | Line 315: | ||
|[[E-Beam Evaporation Recipes#E-Beam 1 .28Sharon.29|R6]] |
|[[E-Beam Evaporation Recipes#E-Beam 1 .28Sharon.29|R6]] |
||
|<br> |
|<br> |
||
|<br> |
|R2<br> |
||
|[[Process Group - Process Control Data#E-Beam 4: Cr|R6]] |
|[[Process Group - Process Control Data#E-Beam 4: Cr|R6]] |
||
|[https://wiki.nanotech.ucsb.edu/w/index.php?title=Sputtering_Recipes#Sputter_3_.28AJA_ATC_2000-F.29 R3] |
|[https://wiki.nanotech.ucsb.edu/w/index.php?title=Sputtering_Recipes#Sputter_3_.28AJA_ATC_2000-F.29 R3] |
||
| Line 365: | Line 365: | ||
! bgcolor="#d0e7ff" align="center" |Ge |
! bgcolor="#d0e7ff" align="center" |Ge |
||
| bgcolor="#eeffff" |[[E-Beam Evaporation Recipes#E-Beam 1 .28Sharon.29|R2]] |
| bgcolor="#eeffff" |[[E-Beam Evaporation Recipes#E-Beam 1 .28Sharon.29|R2]] |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br>R2 |
||
| bgcolor="#eeffff" |[[E-Beam Evaporation Recipes#E-Beam 3 .28Temescal.29|R2]] |
| bgcolor="#eeffff" |[[E-Beam Evaporation Recipes#E-Beam 3 .28Temescal.29|R2]] |
||
| bgcolor="#eeffff" |[[E-Beam Evaporation Recipes#E-Beam 4 .28CHA.29|R2]] |
| bgcolor="#eeffff" |[[E-Beam Evaporation Recipes#E-Beam 4 .28CHA.29|R2]] |
||
| Line 692: | Line 692: | ||
|<br> |
|<br> |
||
|<br> |
|<br> |
||
|[[Sputtering Recipes| |
|[[Sputtering Recipes|R3]] |
||
|<br> |
|<br> |
||
|<br> |
|<br> |
||
| Line 811: | Line 811: | ||
| bgcolor="#eeffff" |[[E-Beam Evaporation Recipes#E-Beam 4 .28CHA.29|R2]] |
| bgcolor="#eeffff" |[[E-Beam Evaporation Recipes#E-Beam 4 .28CHA.29|R2]] |
||
| bgcolor="#eeffff" |[[Sputtering Recipes|R3]] |
| bgcolor="#eeffff" |[[Sputtering Recipes|R3]] |
||
| bgcolor="#eeffff" |[[Sputtering Recipes| |
| bgcolor="#eeffff" |[[Sputtering Recipes|R3]] |
||
| bcolor="EEFFFF" |[[Sputtering Recipes| |
| bcolor="EEFFFF" |[[Sputtering Recipes|R3]] |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| Line 828: | Line 828: | ||
|[[E-Beam Evaporation Recipes#E-Beam 4 .28CHA.29|R2]] |
|[[E-Beam Evaporation Recipes#E-Beam 4 .28CHA.29|R2]] |
||
|<br> |
|<br> |
||
|[[Sputtering Recipes#Ru Deposition .28Sputter 4.29| |
|[[Sputtering Recipes#Ru Deposition .28Sputter 4.29|R3]] |
||
|<br> |
|<br> |
||
|<br> |
|<br> |
||
| Line 840: | Line 840: | ||
|- |
|- |
||
! bgcolor="#d0e7ff" align="center" |Si |
! bgcolor="#d0e7ff" align="center" |Si |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br>R1 |
||
| bgcolor="#eeffff" |[[E-Beam Evaporation Recipes#E-Beam 2 .28Custom.29|R2]] |
| bgcolor="#eeffff" |[[E-Beam Evaporation Recipes#E-Beam 2 .28Custom.29|R2]] |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| Line 1,032: | Line 1,032: | ||
| bgcolor="#eeffff" |[[Process Group - Process Control Data#E-Beam 4: Ti|R6]] |
| bgcolor="#eeffff" |[[Process Group - Process Control Data#E-Beam 4: Ti|R6]] |
||
| bgcolor="#eeffff" |[[Sputtering Recipes|R3]] |
| bgcolor="#eeffff" |[[Sputtering Recipes|R3]] |
||
| bgcolor="#eeffff" |[[Sputtering Recipes| |
| bgcolor="#eeffff" |[[Sputtering Recipes|R3]] |
||
| bgcolor="#eeffff" |[[Sputtering Recipes|R6]] |
| bgcolor="#eeffff" |[[Sputtering Recipes|R6]] |
||
| bgcolor="#eeffff" |R1 |
| bgcolor="#eeffff" |R1 |
||
| Line 1,049: | Line 1,049: | ||
|<br> |
|<br> |
||
|<br> |
|<br> |
||
|[[Sputtering Recipes#Sputter 4 (AJA ATC 2200-V)|R3]] |
|||
|[https://wiki.nanotech.ucsb.edu/w/index.php?title=Sputtering_Recipes#Sputter_4_.28AJA_ATC_2200-V.29 R4] |
|||
|<br> |
|<br> |
||
|R1 |
|R1 |
||
| Line 1,065: | Line 1,065: | ||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| bgcolor="#eeffff" |[ |
| bgcolor="#eeffff" |[[Sputtering Recipes#TiW Co-Sputter Deposition (Sputter 3)|R3]] |
||
| bgcolor="#eeffff" |[[Sputtering Recipes| |
| bgcolor="#eeffff" |[[Sputtering Recipes|R3]] |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| Line 1,083: | Line 1,083: | ||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| bgcolor="#eeffff" |[[Sputtering Recipes|R1]] |
| bgcolor="#eeffff" |[[Sputtering Recipes|R1]] |
||
| bgcolor="#eeffff" |[[Sputtering Recipes| |
| bgcolor="#eeffff" |[[Sputtering Recipes|R3]] |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| bgcolor="#eeffff" |[[Sputtering Recipes#Si3N4 deposition .28IBD.29|R3]] |
| bgcolor="#eeffff" |[[Sputtering Recipes#Si3N4 deposition .28IBD.29|R3]] |
||
| Line 1,095: | Line 1,095: | ||
|- |
|- |
||
! bgcolor="#d0e7ff" align="center" |V |
! bgcolor="#d0e7ff" align="center" |V |
||
| ⚫ | |||
|<br> |
|<br> |
||
|<br> |
|<br> |
||
|<br> |
|<br>R1 |
||
| ⚫ | |||
|[[Sputtering Recipes|R1]] |
|[[Sputtering Recipes|R1]] |
||
|[[Sputtering Recipes|R1]] |
|[[Sputtering Recipes|R1]] |
||
| Line 1,115: | Line 1,115: | ||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |R1<br> |
||
| bgcolor="#eeffff" |[[Sputtering Recipes#TiW Co-Sputter Deposition (Sputter 3)|R3]] |
|||
| bgcolor="#eeffff" |[https://wiki.nanofab.ucsb.edu/w/index.php?title=Sputtering_Recipes&veaction=edit§ion=13 R3] |
|||
| bgcolor="#eeffff" |[[Sputtering Recipes| |
| bgcolor="#eeffff" |[[Sputtering Recipes|R3]] |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| bgcolor="#eeffff" |<br> |
| bgcolor="#eeffff" |<br> |
||
| Line 1,250: | Line 1,250: | ||
|- |
|- |
||
|R4 |
|R4 |
||
| colspan="11" |Process has a documented procedure with regular (≥4x per year) data |
| colspan="11" |Process has a documented procedure with regular (≥4x per year) data '''no''' in-Situ control available |
||
|- |
|- |
||
|R5 |
|R5 |
||
Latest revision as of 06:38, 23 January 2026
Process Control Data
See linked page for process control data (calibration data over time, such as dep. rate, refractive index, stress etc.) over time, for a selection of highly used tools/films.
Deposition Tools/Materials Table
Process Maturity Ranking
R6- most mature process with regular calibrations recorded on SPC charts.- …
R1- least mature - "possible" but you'll have to figure it out.
The Key/Legend for this table's R1...R6 values is at the bottom of the page.
Process Ranking Table
Processes in the table above are ranked by their "Process Maturity Level" as follows:
| Process Level | Description of Process Level Ranking | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| A | Process Allowed and materials available but never done | ||||||||||
| R1 | Process has been ran at least once | ||||||||||
| R2 | Process has been ran and procedure is documented | ||||||||||
| R3 | Process has been ran, procedure is documented, and data is available | ||||||||||
| R4 | Process has a documented procedure with regular (≥4x per year) data no in-Situ control available | ||||||||||
| R5 | Process has a documented procedure with regular (≥4x per year) data and in-Situ control available | ||||||||||
| R6 | Process has a documented procedure and control charts/limits available. Controlled process. | ||||||||||