Dry Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
ficp etch ranking data pt5 |
|||
| Line 882: | Line 882: | ||
==='''Process Ranking Table'''=== |
==='''Process Ranking Table'''=== |
||
{| class="wikitable" |
{| class="wikitable" |
||
!Process Level |
|||
! colspan="11" |Description of Process Level Ranking |
|||
|- |
|- |
||
|A |
|A |
||
Revision as of 16:27, 24 July 2024
Process Control Data
See linked page for process control data (dep rate/stress etc. over time), for a selection of often-used thin-film depositions.
Dry Etching Tools/Materials Table
Process Ranking Table
| Process Level | Description of Process Level Ranking | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| A | Process allowed and materials available but never done | ||||||||||
| R1 | Process has been ran at least once | ||||||||||
| R2 | Process has been ran and/or procedure is documented or/and data available | ||||||||||
| R3 | Process has been ran, procedure is documented, and data is available | ||||||||||
| R4 | Process has a documented procedure with regular (≥4x per year) data or lookahead/in-Situ control available | ||||||||||
| R5 | Process has a documented procedure with regular (≥4x per year) data and lookahead/in-Situ control available | ||||||||||
| R6 | Process has a documented procedure, regular ( ≥4x per year) data, and control charts/limits available | ||||||||||