ICP Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
| Line 3: | Line 3: | ||
==SiO<sub>2</sub> Vertical Etch (Panasonic 1)== |
==SiO<sub>2</sub> Vertical Etch (Panasonic 1)== |
||
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe]] |
*[[media:Panasonic1-SiO-Etch.pdf|SiO<sub>2</sub> Vertical Etch Recipe]] |
||
==SiO<sub>2</sub> Pure CHF3 Etch Recipe Variations (Panasonic 1)== |
|||
*[[media:==SiO<sub>2</sub> Vertical Etch (Panasonic 1)|SiO<sub>2</sub> Vertical Etch Recipe]] |
|||
==Cr Etch (Panasonic 1)== |
==Cr Etch (Panasonic 1)== |
||
Revision as of 18:19, 30 August 2013
Back to Dry Etching Recipes.
ICP Etch 1 (Panasonic E626I)
SiO2 Vertical Etch (Panasonic 1)
SiO2 Pure CHF3 Etch Recipe Variations (Panasonic 1)
- [[media:==SiO2 Vertical Etch (Panasonic 1)|SiO2 Vertical Etch Recipe]]