PECVD Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
| Line 3: | Line 3: | ||
== SiN deposition (PECVD #1) == |
== SiN deposition (PECVD #1) == |
||
*[[media:PECVD1-SiN-standard recipe 1000A.pdf|SiN Standard Recipe]] |
*[[media:PECVD1-SiN-standard recipe 1000A.pdf|SiN Standard Recipe]] |
||
*[[media: |
*[[media:|SiN Data (Deposition rate, Refractive index, Stress, HF etch rate)]] |
||
*[[media:PECVD1 SIN 2-pt Thickness-index uniformity March 2014.pdf|SiN 2-pt thickness and index uniformity]] |
*[[media:PECVD1 SIN 2-pt Thickness-index uniformity March 2014.pdf|SiN 2-pt thickness and index uniformity]] |
||
*[[media:PECVD1 SIN Thickness &index uniformity March 2014.pdf|SiN Thickness and Index uniformity]] |
*[[media:PECVD1 SIN Thickness &index uniformity March 2014.pdf|SiN Thickness and Index uniformity]] |
||
Revision as of 22:33, 20 March 2014
Back to Vacuum Deposition Recipes.
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
- SiN Standard Recipe
- [[media:|SiN Data (Deposition rate, Refractive index, Stress, HF etch rate)]]
- SiN 2-pt thickness and index uniformity
- SiN Thickness and Index uniformity
- SiN Data March 2014
SiO2 deposition (PECVD #1)
SiOxNy deposition (PECVD #1)
PECVD 2 (Advanced Vacuum)
SiN deposition (PECVD #2)
SiO2 deposition (PECVD #2)
Amorphous-Si deposition (PECVD #2)
ICP-PECVD (Unaxis VLR)
SiN deposition (Unaxis VLR)
SiN (2% SiH4)
SiN (2% SiH4 - No-Ar)
| 50° | 100° | 250° |
|---|---|---|
SiN (2% SiH4 - No-Ar - Extra N2)
| 50° | 100° | 250° |
|---|---|---|
SiN (100% SiH4 )
| 50° | 100° | 250° |
|---|---|---|
SiO2 deposition (Unaxis VLR)
SiO2 (2% SiH4)
| 50° | 100° | 250° |
|---|---|---|
SiO2 (2% SiH4 - No Ar)
| 50° | 100° | 250° |
|---|---|---|
SiO2 (100% SiH4 HDR)
| 50° | 100° | 250° |
|---|---|---|
SiO2 (100% SiH4 LDR)
| 50° | 100° | 250° |
|---|---|---|
Amorphous Si (100%SiH4 Ar He)
| 90° | 250° |
|---|---|