PECVD Recipes: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Biljana (talk | contribs)
Biljana (talk | contribs)
Line 10: Line 10:
*[https://docs.google.com/spreadsheets/d/1-pET1Eojooso5UHk90W-5uYByDDdrCyRnggqewxTmVg/edit#gid=sharing SiN 1000A Thickness uniformity 2015]
*[https://docs.google.com/spreadsheets/d/1-pET1Eojooso5UHk90W-5uYByDDdrCyRnggqewxTmVg/edit#gid=sharing SiN 1000A Thickness uniformity 2015]
*[https://docs.google.com/spreadsheets/d/1V_-KzsdR-2tSnJGtUdQWokmnNIY949t0vdQOp7RfCgc/edit#gid=sharing SiN Thickness uniformity 2016]
*[https://docs.google.com/spreadsheets/d/1V_-KzsdR-2tSnJGtUdQWokmnNIY949t0vdQOp7RfCgc/edit#gid=sharing SiN Thickness uniformity 2016]


== LS SiN deposition (PECVD #1) ==
<!-- Placeholders - Not uploaded yet-->
*[[media:New PECVD1-LS SIN-Turner05recipe 2014 LS SIN recipe.pdf|LS SiN Standard Recipe]]
*[https://docs.google.com/spreadsheets/d/1Joz0az9TGZWQc4CiMQJZzLBbNFbx_hH2Oc0B4NNJmYk/edit#gid=sharing LS SiN Data 2014]
*[https://docs.google.com/spreadsheets/d/1xIzc2CufRYNSfAtsOXpw3IzHreeu42BWrLBV0kzP6kA/edit#gid=sharing LS SiN 1000A Thickness uniformity 2014]
<!-- Placeholders - Not uploaded yet-->


== SiO<sub>2</sub> deposition (PECVD #1) ==
== SiO<sub>2</sub> deposition (PECVD #1) ==
Line 28: Line 20:
*[https://docs.google.com/spreadsheets/d/1WUCm_dWpxKTjfFf1rNfLuxvwMxsyCYON_OZ3gb50L_s/edit#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2016]
*[https://docs.google.com/spreadsheets/d/1WUCm_dWpxKTjfFf1rNfLuxvwMxsyCYON_OZ3gb50L_s/edit#gid=sharing SiO<sub>2</sub> 1000A Thickness uniformity 2016]


== LS SiN deposition (PECVD #1) ==
== OTHER recipes LS SiN deposition (PECVD #1) ==
<!-- Placeholders - Not uploaded yet-->
<!-- Placeholders - Not uploaded yet-->
*[[media:New PECVD1-LS SIN-Turner05recipe 2014 LS SIN recipe.pdf|LS SiN Standard Recipe]]
*[[media:New PECVD1-LS SIN-Turner05recipe 2014 LS SIN recipe.pdf|LS SiN Standard Recipe]]

Revision as of 22:22, 8 January 2016

Back to Vacuum Deposition Recipes.

PECVD 1 (PlasmaTherm 790)

SiN deposition (PECVD #1)

SiO2 deposition (PECVD #1)

OTHER recipes LS SiN deposition (PECVD #1)




SiOxNy deposition (PECVD #1)

PECVD 2 (Advanced Vacuum)

SiO2 deposition (PECVD #2)

SiN deposition (PECVD #2)

LS SiN deposition (PECVD #2)

Amorphous-Si deposition (PECVD #2)

ICP-PECVD (Unaxis VLR)

SiN deposition (Unaxis VLR)

SiN (2% SiH4)

50° (pinholes) 100° (pinholes) 250°

SiN (2% SiH4 - No-Ar)

50° (pinholes) 100° (pinholes) 250°

SiN (2% SiH4 - No-Ar - Extra N2)

50° (pinholes) 100° (pinholes) 250°

SiN (100% SiH4 )

50° (pinholes) 100° (pinholes) 250°

SiO2 deposition (Unaxis VLR)

SiO2 (2% SiH4)

50° 100° 250°

SiO2 (2% SiH4 - No Ar)

50° 100° 250°

SiO2 (100% SiH4 HDR)

50° 100° 250°

SiO2 (100% SiH4 LDR)

50° 100° 250°

Amorphous Si (100%SiH4 Ar He)

90° 250°