Dry Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
No edit summary |
ICP2 PR/ARC reipce link |
||
| Line 1: | Line 1: | ||
{{Recipe Table Explanation}} |
{{Recipe Table Explanation}} |
||
{| class="wikitable |
{| class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" border="1" |
||
|- bgcolor="# |
|- bgcolor="#d0e7ff" |
||
! |
! width="725" height="45" colspan="17" | <div style="font-size: 150%;">Dry Etching Recipes</div> |
||
|- bgcolor="# |
|- bgcolor="#d0e7ff" |
||
| <!-- INTENTIONALLY LEFT BLANK --> |
| <!-- INTENTIONALLY LEFT BLANK --> |
||
! |
! width="300" height="35" align="center" bgcolor="#d0e7ff" colspan="4" | '''[[RIE Etching Recipes|RIE Etching]]''' |
||
! colspan="5" |'''[[ICP Etching Recipes|ICP Etching]]''' |
! colspan="5" |'''[[ICP Etching Recipes|ICP Etching]]''' |
||
! |
! align="center" bgcolor="#d0e7ff" colspan="4" |'''[[Oxygen Plasma System Recipes|Oxygen Plasma Systems]]''' |
||
! |
! align="center" bgcolor="#d0e7ff" colspan="3" |'''[[Other Dry Etching Recipes|Other Dry Etchers]]''' |
||
|- |
|- |
||
! width="65" |
! width="65" align="center" bgcolor="#d0e7ff" | '''Material''' |
||
| width="65" bgcolor="# |
| width="65" bgcolor="#daf1ff" | [[RIE 1 (Custom)|RIE 1<br>(Retired)]] |
||
| width="65" bgcolor="# |
| width="65" bgcolor="#daf1ff" | [[RIE_Etching_Recipes#RIE_2_.28MRC.29|RIE 2<br> (MRC)]] |
||
| width="65" bgcolor="# |
| width="65" bgcolor="#daf1ff" | [[RIE_Etching_Recipes#RIE_3_.28MRC.29|RIE 3<br> (MRC)]] |
||
| width="100" bgcolor="# |
| width="100" bgcolor="#daf1ff" | [[RIE_Etching_Recipes#RIE_5_.28PlasmaTherm.29|RIE 5<br>(PlasmaTherm)]] |
||
| width="100" bgcolor="# |
| width="100" bgcolor="#daf1ff" | [[ICP_Etching_Recipes#DSEIII_.28PlasmaTherm.2FDeep_Silicon_Etcher.29|DSEIII<br>(PlasmaTherm)]] |
||
| width="100" bgcolor="# |
| width="100" bgcolor="#daf1ff" | [[ICP_Etching_Recipes#Si_Deep_RIE_.28PlasmaTherm.2FBosch_Etch.29|Si Deep RIE<br>(PTI/Bosch)]] |
||
| width="120" bgcolor="# |
| width="120" bgcolor="#daf1ff" | [[ICP_Etching_Recipes#ICP_Etch_1_.28Panasonic_E626I.29|ICP Etch 1<br>(Panasonic 1)]] |
||
| width="120" bgcolor="# |
| width="120" bgcolor="#daf1ff" | [[ICP_Etching_Recipes#ICP_Etch_2_.28Panasonic_E640.29|ICP Etch 2<br>(Panasonic 2)]] |
||
| width="85" bgcolor="# |
| width="85" bgcolor="#daf1ff" | [[ICP_Etching_Recipes#ICP-Etch_.28Unaxis_VLR.29|ICP-Etch<br>(Unaxis VLR)]] |
||
| width="85" bgcolor="# |
| width="85" bgcolor="#daf1ff" | [[Oxygen_Plasma_System_Recipes#Ashers_.28Technics_PEII.29|Ashers<br>(Technics PEII)]] |
||
| width="95" bgcolor="# |
| width="95" bgcolor="#daf1ff" | [[Oxygen_Plasma_System_Recipes#Plasma_Clean_.28Gasonics_2000.29|Plasma Clean<br>(Gasonics 2000)]] |
||
| width="85" bgcolor="# |
| width="85" bgcolor="#daf1ff" | [[Oxygen_Plasma_System_Recipes#UV_Ozone_Reactor|UV Ozone Reactor]] |
||
| width="85" bgcolor="# |
| width="85" bgcolor="#daf1ff" | [[Oxygen_Plasma_System_Recipes#Plasma_Activation_.28EVG_810.29|Plasma Activation<br>(EVG 810)]] |
||
| width="85" bgcolor="# |
| width="85" bgcolor="#daf1ff" | [[Other_Dry_Etching_Recipes#XeF2_Etch_.28Xetch.29|XeF2 Etch<br>(Xetch)]] |
||
| width="85" bgcolor="# |
| width="85" bgcolor="#daf1ff" | [[Other_Dry_Etching_Recipes#Vapor_HF_Etch_.28uETCH.29|Vapor HF Etch<br>(uETCH)]] |
||
| width="85" bgcolor="# |
| width="85" bgcolor="#daf1ff" | [[Other_Dry_Etching_Recipes#CAIBE_.28Oxford_Ion_Mill.29|CAIBE<br>(Oxford)]] |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | Ag |
||
| |
| |
||
| |
| |
||
| Line 45: | Line 45: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | Al |
||
| |
| |
||
| |
| |
||
| Line 63: | Line 63: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | Au |
||
| |
| |
||
| |
| |
||
| Line 81: | Line 81: | ||
| |
| |
||
|{{rl|Other Dry Etching Recipes|Other Dry Etch (CAIBE (Oxford Ion Mill))}} |
|{{rl|Other Dry Etching Recipes|Other Dry Etch (CAIBE (Oxford Ion Mill))}} |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | Cr |
||
| |
| |
||
| |
| |
||
| Line 99: | Line 99: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | Cu |
||
| |
| |
||
| |
| |
||
| Line 118: | Line 118: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | Ge |
||
| |
| |
||
| |
| |
||
| Line 135: | Line 135: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | Mo |
||
| |
| |
||
| |
| |
||
| Line 154: | Line 154: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | Ni |
||
| |
| |
||
| |
| |
||
| Line 172: | Line 172: | ||
|{{rl|Other Dry Etching Recipes|Other Dry Etch (CAIBE (Oxford Ion Mill))}} |
|{{rl|Other Dry Etching Recipes|Other Dry Etch (CAIBE (Oxford Ion Mill))}} |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | Pt |
||
| |
| |
||
| |
| |
||
| Line 190: | Line 190: | ||
|{{rl|Other Dry Etching Recipes|Other Dry Etch (CAIBE (Oxford Ion Mill))}} |
|{{rl|Other Dry Etching Recipes|Other Dry Etch (CAIBE (Oxford Ion Mill))}} |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | Ru |
||
| |
| |
||
| |
| |
||
| Line 207: | Line 207: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | Si |
||
| |
| |
||
| |
| |
||
| Line 226: | Line 226: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | Ta |
||
| |
| |
||
| |
| |
||
| Line 244: | Line 244: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | Ti |
||
| |
| |
||
| |
| |
||
| Line 262: | Line 262: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | Al<sub>2</sub>O<sub>3</sub> |
||
| |
| |
||
| |
| |
||
| Line 279: | Line 279: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | Al<sub>2</sub>O<sub>3 (Sapphire)</sub> |
||
| |
| |
||
| |
| |
||
| Line 298: | Line 298: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | AlGaAs |
||
| |
| |
||
| |
| |
||
| Line 315: | Line 315: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | AlGaN |
||
| |
| |
||
| |
| |
||
| Line 334: | Line 334: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | AlN |
||
| |
| |
||
| |
| |
||
| Line 351: | Line 351: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | CdZnTe |
||
| |
| |
||
| {{rl|RIE Etching Recipes|CdZnTe Etch (RIE 2)}} |
| {{rl|RIE Etching Recipes|CdZnTe Etch (RIE 2)}} |
||
| Line 369: | Line 369: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | GaAs |
||
| |
| |
||
| |
| |
||
| Line 388: | Line 388: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | GaN |
||
| |
| |
||
| |
| |
||
| Line 405: | Line 405: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | GaSb |
||
| |
| |
||
| |
| |
||
| Line 423: | Line 423: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | HfO<sub>2</sub> |
||
| |
| |
||
| |
| |
||
| Line 441: | Line 441: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | InGaAlAs |
||
| |
| |
||
| {{rl|RIE Etching Recipes|RIE 2 (MRC)|InP-InGaAsP-InGaAlAs Etching (RIE 2)|InP Etch (RIE 2)}} |
| {{rl|RIE Etching Recipes|RIE 2 (MRC)|InP-InGaAsP-InGaAlAs Etching (RIE 2)|InP Etch (RIE 2)}} |
||
| Line 460: | Line 460: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | InGaAsP |
||
| |
| |
||
| {{rl|RIE Etching Recipes|RIE 2 (MRC)|InP-InGaAsP-InGaAlAs Etching (RIE 2)|InP Etch (RIE 2)}} |
| {{rl|RIE Etching Recipes|RIE 2 (MRC)|InP-InGaAsP-InGaAlAs Etching (RIE 2)|InP Etch (RIE 2)}} |
||
| Line 477: | Line 477: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | InP |
||
| |
| |
||
| {{rl|RIE Etching Recipes|RIE 2 (MRC)|InP-InGaAsP-InGaAlAs Etching (RIE 2)|InP Etch (RIE 2)}} |
| {{rl|RIE Etching Recipes|RIE 2 (MRC)|InP-InGaAsP-InGaAlAs Etching (RIE 2)|InP Etch (RIE 2)}} |
||
| Line 496: | Line 496: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | ITO |
||
| |
| |
||
| {{rl|RIE Etching Recipes|ITO Etch (RIE 2)}} |
| {{rl|RIE Etching Recipes|ITO Etch (RIE 2)}} |
||
| Line 513: | Line 513: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
!Photoresist |
!Photoresist |
||
& ARC |
& ARC |
||
| Line 523: | Line 523: | ||
| |
| |
||
|A |
|A |
||
|[https://www.nanotech.ucsb.edu/wiki/index.php/ICP_Etching_Recipes#Photoresist_and_ARC_etching R] |
|||
|A |
|||
| |
| |
||
|A |
|A |
||
| Line 533: | Line 533: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | SiC |
||
| |
| |
||
| |
| |
||
| Line 551: | Line 551: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | SiN |
||
| |
| |
||
| |
| |
||
| Line 568: | Line 568: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | SiO<sub>2</sub> |
||
| |
| |
||
| |
| |
||
| Line 586: | Line 586: | ||
| {{rl|Other Dry Etching Recipes|Other Dry Etch (Vapor HF Etcher)}} |
| {{rl|Other Dry Etching Recipes|Other Dry Etch (Vapor HF Etcher)}} |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | SiOxNy |
||
| |
| |
||
| |
| |
||
| Line 605: | Line 605: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | Ta<sub>2</sub>O<sub>5</sub> |
||
| |
| |
||
| |
| |
||
| Line 623: | Line 623: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | TiN |
||
| |
| |
||
| |
| |
||
| Line 640: | Line 640: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | TiO<sub>2</sub> |
||
| |
| |
||
| |
| |
||
| Line 658: | Line 658: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | W-TiW |
||
| |
| |
||
| |
| |
||
| Line 676: | Line 676: | ||
| |
| |
||
| |
| |
||
|- bgcolor="# |
|- bgcolor="#eeffff" |
||
! |
! align="center" bgcolor="#d0e7ff" | ZnO<sub>2</sub> |
||
| |
| |
||
| |
| |
||
| Line 695: | Line 695: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | ZnS |
||
| |
| |
||
| {{rl|RIE Etching Recipes|ZnS Etching (RIE 2)}} |
| {{rl|RIE Etching Recipes|ZnS Etching (RIE 2)}} |
||
| Line 713: | Line 713: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | ZnSe |
||
| |
| |
||
| {{rl|RIE Etching Recipes|ZnS Etching (RIE 2)}} |
| {{rl|RIE Etching Recipes|ZnS Etching (RIE 2)}} |
||
| Line 731: | Line 731: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | ZrO<sub>2</sub> |
||
| |
| |
||
| |
| |
||
| Line 749: | Line 749: | ||
| |
| |
||
|- |
|- |
||
! |
! align="center" bgcolor="#d0e7ff" | '''Material''' |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[RIE 1 (Custom)|RIE 1<br>(Retired)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[RIE_Etching_Recipes#RIE_2_.28MRC.29|RIE 2<br> (MRC)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[RIE_Etching_Recipes#RIE_3_.28MRC.29|RIE 3<br> (MRC)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[RIE_Etching_Recipes#RIE_5_.28PlasmaTherm.29|RIE 5<br>(PlasmaTherm)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[ICP_Etching_Recipes#DSEIII_.28PlasmaTherm.2FDeep_Silicon_Etcher.29|DSEIII<br>(PlasmaTherm)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[ICP_Etching_Recipes#Si_Deep_RIE_.28PlasmaTherm.2FBosch_Etch.29|Si Deep RIE<br>(PlasmaTherm/Bosch Etch)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[ICP_Etching_Recipes#ICP_Etch_1_.28Panasonic_E626I.29|ICP Etch 1<br>(Panasonic E626I)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[ICP_Etching_Recipes#ICP_Etch_2_.28Panasonic_E640.29|ICP Etch 2<br>(Panasonic E640)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[ICP_Etching_Recipes#ICP-Etch_.28Unaxis_VLR.29|ICP-Etch<br>(Unaxis VLR)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[Oxygen_Plasma_System_Recipes#Ashers_.28Technics_PEII.29|Ashers<br>(Technics PEII)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[Oxygen_Plasma_System_Recipes#Plasma_Clean_.28Gasonics_2000.29|Plasma Clean<br>(Gasonics 2000)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[Oxygen_Plasma_System_Recipes#UV_Ozone_Reactor|UV Ozone Reactor]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[Oxygen_Plasma_System_Recipes#Plasma_Activation_.28EVG_810.29|Plasma Activation<br>(EVG 810)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[Other_Dry_Etching_Recipes#XeF2_Etch_.28Xetch.29|XeF2 Etch<br>(Xetch)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[Other_Dry_Etching_Recipes#Vapor_HF_Etch_.28uETCH.29|Vapor HF Etch<br>(uETCH)]] |
||
| bgcolor="# |
| bgcolor="#daf1ff" | [[Other_Dry_Etching_Recipes#CAIBE_.28Oxford_Ion_Mill.29|CAIBE<br>(Oxford)]] |
||
|} |
|} |
||
Revision as of 20:44, 16 March 2018
- R = Recipe is available. Clicking this link will take you to the recipe.
- A = Material is available for use, but no recipes are provided.