Vacuum Deposition Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
No edit summary |
link to process control data |
||
| Line 1: | Line 1: | ||
=== [[Process Group - Process Control Data#Deposition .28Process Control Data.29|<u>Process Control Data</u>]] === |
|||
See [[Process Group - Process Control Data#Deposition .28Process Control Data.29|linked page]] for process control data (calibration data over time, such as dep. rate, refractive index, stress etc.) over time, for a selection of highly used tools/films. |
|||
=== Deposition Tools/Materials Table === |
|||
{{Recipe Table Explanation}} |
{{Recipe Table Explanation}} |
||
{| class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;" border="1" |
{| class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;" border="1" |
||
|- bgcolor="#d0e7ff" |
|- bgcolor="#d0e7ff" |
||
Revision as of 22:55, 8 June 2022
Process Control Data
See linked page for process control data (calibration data over time, such as dep. rate, refractive index, stress etc.) over time, for a selection of highly used tools/films.
Deposition Tools/Materials Table
- R = Recipe is available. Clicking this link will take you to the recipe.
- A = Material is available for use, but no recipes are provided.