Wafer Bonder (SUSS SB6-8E): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Silva (talk | contribs)
No edit summary
Line 12: Line 12:
|toolid=41
|toolid=41
}}
}}
= About =
=About=
This is Karl-Suss model SB-6 substrate bonder. Wafer bonding of pieces to 6” wafers can be done at pressures from 5e-5 to 3e3 mBar and from 50°C to 550°C. This tool mates with the Karl-Suss MA-6 aligner to allow for aligned bonding. Forces up to 20 kN for a 150 mm wafer size are available. The system supports thermal compression as well as anodic bonding (up to 2000 V). The system is computer controlled with a windows environment allowing for multiple recipe steps and saving of recipes and data. The system is configured for manual loading of wafers.
This is Karl-Suss model SB-6 substrate bonder. Wafer bonding of pieces to 6” wafers can be done at pressures from 5e-5 to 3e3 mBar and from 50°C to 550°C. This tool mates with the Karl-Suss MA-6 aligner to allow for aligned bonding. Forces up to 20 kN for a 150 mm wafer size are available. The system supports thermal compression as well as anodic bonding (up to 2000 V). The system is computer controlled with a windows environment allowing for multiple recipe steps and saving of recipes and data. The system is configured for manual loading of wafers.


=Detailed Specifications=
=Detailed Specifications=

*Wafer bonding from 50°C to 550°C, +/- 5 degrees accuracy, +/- 3% uniformity
*Wafer bonding from 50°C to 550°C, +/- 5 degrees accuracy, +/- 3% uniformity
*Upper and lower heating of samples
*Upper and lower heating of samples
*5e-5 to 3e3 Torr environment bonding pressure, with Nitrogen
*5e-5 to 3e3 Torr environment bonding pressure, with Nitrogen
*Sample size: pieces to 6” wafers, aligned bonding by using MA/BA-6 aligner
*Sample size: pieces to 6” wafers, aligned bonding by using the [[Contact Aligner (SUSS MA-6)|MA/BA-6 aligner]] - contact supervisor for setup.
*Anodic bonding to 2000 V
*Anodic bonding to 2000 V
*Windows-based computer control
*Windows-based computer control

Revision as of 01:53, 4 January 2023

Wafer Bonder (SUSS SB6-8E)
Location Bay 7
Tool Type Thermal Processing
Manufacturer Karl Suss America
Description Karl Suss Substrate Bonder

Primary Supervisor Aidan Hopkins
(805) 893-2343
hopkins@ece.ucsb.edu

Secondary Supervisor

Lee Sawyer


Recipes

SignupMonkey: Sign up for this tool


About

This is Karl-Suss model SB-6 substrate bonder. Wafer bonding of pieces to 6” wafers can be done at pressures from 5e-5 to 3e3 mBar and from 50°C to 550°C. This tool mates with the Karl-Suss MA-6 aligner to allow for aligned bonding. Forces up to 20 kN for a 150 mm wafer size are available. The system supports thermal compression as well as anodic bonding (up to 2000 V). The system is computer controlled with a windows environment allowing for multiple recipe steps and saving of recipes and data. The system is configured for manual loading of wafers.

Detailed Specifications

  • Wafer bonding from 50°C to 550°C, +/- 5 degrees accuracy, +/- 3% uniformity
  • Upper and lower heating of samples
  • 5e-5 to 3e3 Torr environment bonding pressure, with Nitrogen
  • Sample size: pieces to 6” wafers, aligned bonding by using the MA/BA-6 aligner - contact supervisor for setup.
  • Anodic bonding to 2000 V
  • Windows-based computer control
  • Wafer bonder currently set up for 4" wafers