Wafer Bonder (SUSS SB6-8E): Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
→Detailed Specifications: link to MA6 |
No edit summary |
||
| Line 24: | Line 24: | ||
*Windows-based computer control |
*Windows-based computer control |
||
*Wafer bonder currently set up for 4" wafers |
*Wafer bonder currently set up for 4" wafers |
||
=Documentation= |
|||
*Bonder Pressure Rules Visual Aid |
|||
*Bonder Recipe Guidelines |
|||
Revision as of 14:24, 20 September 2023
| ||||||||||||||||||||||||||||||
About
This is Karl-Suss model SB-6 substrate bonder. Wafer bonding of pieces to 6” wafers can be done at pressures from 5e-5 to 3e3 mBar and from 50°C to 550°C. This tool mates with the Karl-Suss MA-6 aligner to allow for aligned bonding. Forces up to 20 kN for a 150 mm wafer size are available. The system supports thermal compression as well as anodic bonding (up to 2000 V). The system is computer controlled with a windows environment allowing for multiple recipe steps and saving of recipes and data. The system is configured for manual loading of wafers.
Detailed Specifications
- Wafer bonding from 50°C to 550°C, +/- 5 degrees accuracy, +/- 3% uniformity
- Upper and lower heating of samples
- 5e-5 to 3e3 Torr environment bonding pressure, with Nitrogen
- Sample size: pieces to 6” wafers, aligned bonding by using the MA/BA-6 aligner - contact supervisor for setup.
- Anodic bonding to 2000 V
- Windows-based computer control
- Wafer bonder currently set up for 4" wafers
Documentation
- Bonder Pressure Rules Visual Aid
- Bonder Recipe Guidelines