We were able to fix the vacuum leak but unfortunately the particulates are off the chart and rate is still a bit low. Tomorrow morning we will be taking the showerhead apart and cleaning it up before testing again.
Initially it was planned to remove the hoist again to rebuild it to solve the leak.
⚫
//[[User:Mehalana v|Vraj Mehalana]] 16:48, 31 October 2023 (PDT)

The manufacturer is sending out a rebuild kit under warranty since it is a brand new hoist that is leaking.
When that arrives I will schedule another all day event to rebuild the hoist.

I cleaned up the leaked oil, checked oil level, and did an inspection of the tool.
System is back up and available for use.

⚫
//[[User:Mehalana v|Vraj Mehalana]] 11:11, 23 October 2023 (PDT)
=====Unaxis VLR - GapFill allowed Mon 30th 5pm to Wed 6am=====
=====Unaxis VLR - GapFill allowed Mon 30th 5pm to Wed 6am=====
We are still working on an improved GapFill recipe.
We are still working on an improved GapFill recipe.

Revision as of 23:48, 31 October 2023

Job Opening: Process Engineer

The Nanofab has a current job opening for a Process/Wafer-Fab Engineer, see the NanoFab Job Openings page for details. //Vraj Mehalana 14:52, 30 October 2023 (PDT)

EBeam2 UP

Test run completed without issue. System is ready to use, EXCEPT for heater - contact supervisor for heater use. See email for updates to operating procedure.

//Vraj Mehalana 11:48, 26 October 2023 (PDT)

ProbeStation scheduled IT maintenance

The ProbeStation will be undergoing IT maintenance and will be unavailable on the following dates :

  • 10-30-23
  • 10-31-23
  • 11-01-23
  • 11-02-23

Please plan your work activities accordingly.

//Vraj Mehalana 14:52, 30 October 2023 (PDT)

PECVD2 is UP

We were able to fix the vacuum leak but unfortunately the particulates are off the chart and rate is still a bit low. Tomorrow morning we will be taking the showerhead apart and cleaning it up before testing again. //Vraj Mehalana 16:48, 31 October 2023 (PDT)

Unaxis VLR - GapFill allowed Mon 30th 5pm to Wed 6am

We are still working on an improved GapFill recipe.

To allow your processes through, on Monday EVENING at 5pm we will allow the old "450W GapFill" recipe to be run,

- starting Monday Oct 30th, evening at 5pm,

- ending Wed Nov 1st, morning at 6am.

Reminder: You may NOT run the 450W recipe outside these allowed times, and you may Not modify our recipes apart from Dep/Clean TIME.

Let me know if you have any questions.

//Vraj Mehalana 09:55, 11 October 2023 (PDT)

Wafer Bonder, (Suss SB6-8E)

The top heater has failed. We are currently in the process of trying to source a new heater. we will send out an email once I have an update.

//Vraj Mehalana 09:59, 20 September 2023 (PDT)

EVG Activation: Up

The FSE has completed the work on the tool and I have made several test runs without issue.

IMPORTANT - Please see corresponding email for changes in operation.

//Vraj Mehalana 15:58, 24 October 2023 (PDT)