Template:Announcements: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
removed qhitespac and internal comments (since vraj's script was pushing them to the bottom, instead of top where they used to be for human-readable instructions))
No edit summary
Line 13: Line 13:


=====PECVD2 is down=====
=====PECVD2 is down=====
Unfortunately PECVD2 is still down.
We were able to fix the vacuum leak but unfortunately the particulates are off the chart and rate is still a bit low. Tomorrow morning we will be taking the showerhead apart and cleaning it up before testing again.

//[[User:Mehalana v|Vraj Mehalana]] 16:48, 31 October 2023 (PDT)
We replaced the MFC and ran into devicenet issues.
I swapped the internal board with the old MFC and the devicenet issues appeared to be resolved.
After another test run, there was no change in dep rate.

We will continue trouble shooting on Monday.
//[[User:Mehalana v|Vraj Mehalana]] 11:08, 12 November 2023 (PST)


=====Wafer Bonder, (Suss SB6-8E)=====
=====Wafer Bonder, (Suss SB6-8E)=====

Revision as of 19:08, 12 November 2023

Job Opening: Process Engineer

The Nanofab has a current job opening for a Process/Wafer-Fab Engineer, see the NanoFab Job Openings page for details. //Vraj Mehalana 14:52, 30 October 2023 (PDT)

Lab Access Changes: Symmetry App

Card/Iris scanner access is still currently enabled. However we will be moving to a smartphone-based access system. IMPORTANT: check your email to setup the new smartphone access system, so you will be ready when we switch to the new system. Look for an email titled "Invitation to Access Symmetry App". // John d 13:49, 7 November 2023 (PST)

ProbeStation scheduled IT maintenance

The probe station is up, only the computer is down. Standard electrical probe measurements are still available, just not automated plotting //Vraj Mehalana 14:29, 3 November 2023 (PDT)

PECVD2 is down

Unfortunately PECVD2 is still down.

We replaced the MFC and ran into devicenet issues. I swapped the internal board with the old MFC and the devicenet issues appeared to be resolved. After another test run, there was no change in dep rate.

We will continue trouble shooting on Monday. //Vraj Mehalana 11:08, 12 November 2023 (PST)

Wafer Bonder, (Suss SB6-8E)

The top heater has failed. We are currently in the process of trying to source a new heater. we will send out an email once I have an update.

//Vraj Mehalana 09:59, 20 September 2023 (PDT)