Dry Etching Recipes: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
Added R6 for GaAs etch on ICP2 |
updated FL-ICP Si + SIO2 link cuz changed header title |
||
| Line 226: | Line 226: | ||
| |
| |
||
|[[ICP Etching Recipes#DSEIII .28PlasmaTherm.2FDeep Silicon Etcher.29|R6]] |
|[[ICP Etching Recipes#DSEIII .28PlasmaTherm.2FDeep Silicon Etcher.29|R6]] |
||
|[[ICP Etching Recipes#Si |
|[[ICP Etching Recipes#Si Etch Recipes (Fluorine ICP Etcher)|R6]] |
||
| |
| |
||
| |
| |
||
| Line 626: | Line 626: | ||
| |
| |
||
| |
| |
||
|[[ICP Etching Recipes#SiO2 |
|[[ICP Etching Recipes#SiO2 Etch Recipes (Fluorine ICP Etcher)|R6]] |
||
|{{rl|ICP Etching Recipes|SiO2 Etching (Panasonic 1)}} |
|{{rl|ICP Etching Recipes|SiO2 Etching (Panasonic 1)}} |
||
|[[ICP Etching Recipes#SiO2 Etching .28Panasonic 2.29|R6]] |
|[[ICP Etching Recipes#SiO2 Etching .28Panasonic 2.29|R6]] |
||
Revision as of 18:55, 9 March 2025
Process Control Data
See above linked page for process control data (dep rate/stress etc. over time), for a selection of often-used dry etches
Dry Etching Tools/Materials Table
The Key/Legend for this table's A...R6 values is at the bottom of the page.
Process Ranking Table
Processes in the table above are ranked by their "Process Maturity Level" as follows:
| Process Level | Description of Process Level Ranking | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| A | Process Allowed and materials available but never done | ||||||||||
| R1 | Process has been run at least once | ||||||||||
| R2 | Process has been run and/or procedure is documented or/and data available | ||||||||||
| R3 | Process has been run, procedure is documented, and data is available | ||||||||||
| R4 | Process has a documented procedure with regular (≥4x per year) data or lookahead/in-situ control available | ||||||||||
| R5 | Process has a documented procedure with regular (≥4x per year) data and lookahead/in-situ control available | ||||||||||
| R6 | Process has a documented procedure, regular ( ≥4x per year) data, and control charts & limits available | ||||||||||