PECVD Recipes: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Biljana (talk | contribs)
Biljana (talk | contribs)
Line 12: Line 12:


== SiO<sub>2</sub> deposition (PECVD #1) ==
== SiO<sub>2</sub> deposition (PECVD #1) ==
*[[media:PECVD1-SiO2-Recipe.pdf|SiO<sub>2</sub> Deposition Recipe]]
*[[media:|SiO<sub>2</sub> Deposition Recipe]]
*[[media:PECVD1- SiO2 Calibratiion February 2014-1 SiO2 1000A.pdf|SiO<sub>2</sub> Calibration February 2014]]
*[[media:PECVD1 SiO2 Data-March 2014 SiO2 Data.pdf|SiO<sub>2</sub> SiO2 Data March2014]]


*[[media:PECVD1-SiO2-Data.pdf|SiO<sub>2</sub> Deposition Particle Thickness Data]]
*[[media:PECVD1-SiO2-Data.pdf|SiO<sub>2</sub> Deposition Particle Thickness Data]]



Revision as of 19:06, 21 March 2014

Back to Vacuum Deposition Recipes.

PECVD 1 (PlasmaTherm 790)

SiN deposition (PECVD #1)

SiO2 deposition (PECVD #1)


SiOxNy deposition (PECVD #1)

PECVD 2 (Advanced Vacuum)

SiN deposition (PECVD #2)

SiO2 deposition (PECVD #2)

Amorphous-Si deposition (PECVD #2)

ICP-PECVD (Unaxis VLR)

SiN deposition (Unaxis VLR)

SiN (2% SiH4)

50° 100° 250°

SiN (2% SiH4 - No-Ar)

50° 100° 250°

SiN (2% SiH4 - No-Ar - Extra N2)

50° 100° 250°

SiN (100% SiH4 )

50° 100° 250°

SiO2 deposition (Unaxis VLR)

SiO2 (2% SiH4)

50° 100° 250°

SiO2 (2% SiH4 - No Ar)

50° 100° 250°

SiO2 (100% SiH4 HDR)

50° 100° 250°

SiO2 (100% SiH4 LDR)

50° 100° 250°

Amorphous Si (100%SiH4 Ar He)

90° 250°