PECVD Recipes: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Biljana (talk | contribs)
Biljana (talk | contribs)
Line 4: Line 4:
*[[media:PECVD1-SiN-1000A Standard recipe.pdf|SiN Standard Recipe]]
*[[media:PECVD1-SiN-1000A Standard recipe.pdf|SiN Standard Recipe]]
*[[media:PECVD1 SIN Data-March 2014 SIN data.pdf|SiN Data (Deposition rate, Refractive index, Stress, HF etch rate)]]
*[[media:PECVD1 SIN Data-March 2014 SIN data.pdf|SiN Data (Deposition rate, Refractive index, Stress, HF etch rate)]]
⚫
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dGtRLWROZGFONTBpLVBNRGQyU3Mxa2c&usp=drive_web#gid=sharing SiN 1000A Thickness uniformity 2014]
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDkyQmFVXzQxbEJPRnFwNWlyVURwbGc&usp=drive_web#gid=sharing SiN Data March 2014]
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dDkyQmFVXzQxbEJPRnFwNWlyVURwbGc&usp=drive_web#gid=sharing SiN Data March 2014]
⚫
*[https://docs.google.com/spreadsheet/ccc?key=0AnwBU1s4JQo2dGtRLWROZGFONTBpLVBNRGQyU3Mxa2c&usp=drive_web#gid=sharing SiN 1000A Thickness uniformity 2014]

<!-- Placeholders - Not uploaded yet-->
<!-- Placeholders - Not uploaded yet-->
* [[media:PECVD1-SiON-Recipe.pdf|Low Stress Si<sub>3</sub>N<sub>4</sub> - Variable Stress Recipes]]
* [[media:PECVD1-SiON-Recipe.pdf|Low Stress Si<sub>3</sub>N<sub>4</sub> - Variable Stress Recipes]]

Revision as of 01:13, 22 March 2014

Back to Vacuum Deposition Recipes.

PECVD 1 (PlasmaTherm 790)

SiN deposition (PECVD #1)

SiO2 deposition (PECVD #1)

SiOxNy deposition (PECVD #1)

PECVD 2 (Advanced Vacuum)

SiN deposition (PECVD #2)

SiO2 deposition (PECVD #2)

Amorphous-Si deposition (PECVD #2)

ICP-PECVD (Unaxis VLR)

SiN deposition (Unaxis VLR)

SiN (2% SiH4)

50° 100° 250°

SiN (2% SiH4 - No-Ar)

50° 100° 250°

SiN (2% SiH4 - No-Ar - Extra N2)

50° 100° 250°

SiN (100% SiH4 )

50° 100° 250°

SiO2 deposition (Unaxis VLR)

SiO2 (2% SiH4)

50° 100° 250°

SiO2 (2% SiH4 - No Ar)

50° 100° 250°

SiO2 (100% SiH4 HDR)

50° 100° 250°

SiO2 (100% SiH4 LDR)

50° 100° 250°

Amorphous Si (100%SiH4 Ar He)

90° 250°