File:UCSBTEST1.png

From UCSB Nanofab Wiki
Revision as of 19:56, 21 March 2023 by John d (talk | contribs) (John d uploaded a new version of File:UCSBTEST1.png)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

Original file (2,479 × 1,991 pixels, file size: 6.52 MB, MIME type: image/png)

test1

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current19:56, 21 March 2023Thumbnail for version as of 19:56, 21 March 20232,479 × 1,991 (6.52 MB)John d (talk | contribs)Typical Recipe UCSB Gain2 for larger particulates
15:19, 7 April 2020Thumbnail for version as of 15:19, 7 April 2020800 × 565 (611 KB)Biljana (talk | contribs)

The following page uses this file:

Metadata