Vacuum Deposition Recipes
E-Beam Evaporation
Sputtering
Thermal Evaporation
Plasma Enhanced Chemical
Vapor Deposition (PECVD)
Atomic Layer Deposition
Ion Beam Deposition (IBD)
Molecular Vapor Deposition
Material
E-Beam 1 (Sharon)
E-Beam 2 (Custom)
E-Beam 3 (Temescal)
E-Beam 4 (CHA)
Sputter 1 (Custom)
Sputter 2
(SFI Endeavor)
Sputter 3
(ATC 2000-F)
Sputter 4
(ATC 2200-V)
Sputter 5 (Lesker AXXIS)
Thermal Evap 1
Thermal Evap 2 (Solder)
PECVD 1
(PlasmaTherm 790)
PECVD 2
(Advanced Vacuum)
Unaxis VLR ICP-PECVD
Atomic Layer Deposition (Tool)
Ion Beam
Deposition (Tool)
Molecular Vapor Deposition (Tool)
Ag
Al
Al
2
O
3
AlN
Au
B
Co
Cr
Cu
Fe
Ge
Hf
HfO
2
In
Ir
ITO
Mo
Nb
Ni
Pd
Pt
Ru
Si
SiN
Y
Y
SiO
2
Y
Y
SiO
x
N
y
Sn
SrF
2
Ta
Ta
2
O
5
Ti
TiN
TiO
2
V
W
Zn
ZnO
2
Zr
ZrO
2
Material
E-Beam 1 (Sharon)
E-Beam 2 (Custom)
E-Beam 3 (Temescal)
E-Beam 4 (CHA)
Sputter 1 (Custom)
Sputter 2
(SFI Endeavor)
Sputter 3
(ATC 2000-F)
Sputter 4
(ATC 2200-V)
Sputter 5 (Lesker AXXIS)
Thermal Evap 1
Thermal Evap 2 (Solder)
PECVD 1
(PlasmaTherm 790)
PECVD 2
(Advanced Vacuum)
Unaxis VLR ICP-PECVD
Atomic Layer Deposition (Tool)
Ion Beam
Deposition (Tool)
Molecular Vapor Deposition (Tool)
Navigation menu
Personal tools
Create account
Log in
Namespaces
Page
Discussion
English
Views
Read
View source
View history
More
Search
InvisibleMenu
QuickLinks
Lab Rules
Common Questions/FAQ
Staff List
Equipment Signup
Chemicals + MSDS
Protofab
Equipment
Full Tool List
Lithography
Vacuum Deposition
Dry Etch
Wet Processing
Thermal Processing
Packaging
Metrology & Test
Recipes and Data
Lithography
Vacuum Deposition
Dry Etching
Wet Etching
Thermal Processing
Packaging Tools
Data + Info
Process Control Data
Tutorials
Calculators/Utilities
NanoFab Info
Research + Pubs
Tech Talks
Tools
What links here
Related changes
Special pages
Printable version
Permanent link
Page information