Difference between revisions of "Wafer Bonder (SUSS SB6-8E)"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
 
(7 intermediate revisions by 4 users not shown)
Line 1: Line 1:
{{tool|{{PAGENAME}}
+
{{tool2|{{PAGENAME}}
 
|picture=WaferBonder.jpg
 
|picture=WaferBonder.jpg
 
|type = Thermal Processing
 
|type = Thermal Processing
|super= Don Freeborn
+
|super= Aidan Hopkins
  +
|super2= Lee Sawyer
 
|phone=(805)839-3918x216
 
|phone=(805)839-3918x216
 
|location=Bay 7
 
|location=Bay 7
Line 11: Line 12:
 
|toolid=41
 
|toolid=41
 
}}
 
}}
= About =
+
=About=
 
This is Karl-Suss model SB-6 substrate bonder. Wafer bonding of pieces to 6” wafers can be done at pressures from 5e-5 to 3e3 mBar and from 50°C to 550°C. This tool mates with the Karl-Suss MA-6 aligner to allow for aligned bonding. Forces up to 20 kN for a 150 mm wafer size are available. The system supports thermal compression as well as anodic bonding (up to 2000 V). The system is computer controlled with a windows environment allowing for multiple recipe steps and saving of recipes and data. The system is configured for manual loading of wafers.
 
This is Karl-Suss model SB-6 substrate bonder. Wafer bonding of pieces to 6” wafers can be done at pressures from 5e-5 to 3e3 mBar and from 50°C to 550°C. This tool mates with the Karl-Suss MA-6 aligner to allow for aligned bonding. Forces up to 20 kN for a 150 mm wafer size are available. The system supports thermal compression as well as anodic bonding (up to 2000 V). The system is computer controlled with a windows environment allowing for multiple recipe steps and saving of recipes and data. The system is configured for manual loading of wafers.
   
 
=Detailed Specifications=
 
=Detailed Specifications=
  +
 
*Wafer bonding from 50°C to 550°C, +/- 5 degrees accuracy, +/- 3% uniformity
 
*Wafer bonding from 50°C to 550°C, +/- 5 degrees accuracy, +/- 3% uniformity
 
*Upper and lower heating of samples
 
*Upper and lower heating of samples
 
*5e-5 to 3e3 Torr environment bonding pressure, with Nitrogen
 
*5e-5 to 3e3 Torr environment bonding pressure, with Nitrogen
*Sample size: pieces to 6” wafers, aligned bonding by using MA/BA-6 aligner
+
*Sample size: pieces to 6” wafers, aligned bonding by using the [[Contact Aligner (SUSS MA-6)|MA/BA-6 aligner]] - contact supervisor for setup.
 
*Anodic bonding to 2000 V
 
*Anodic bonding to 2000 V
 
*Windows-based computer control
 
*Windows-based computer control
  +
*Wafer bonder currently set up for 4" wafers
  +
  +
=Documentation=
  +
  +
*[https://wiki.nanofab.ucsb.edu/w/images/1/12/Bonder_Pressure_Rules_Vis_Aid.docx Bonder Pressure Rules Visual Aid]
  +
*[https://wiki.nanofab.ucsb.edu/w/images/5/5c/Suss_Bonder_Recipe_Guidelines.docx Bonder Recipe Guidelines]

Latest revision as of 10:53, 20 September 2023

Wafer Bonder (SUSS SB6-8E)
WaferBonder.jpg
Location Bay 7
Tool Type Thermal Processing
Manufacturer Karl Suss America
Description Karl Suss Substrate Bonder

Primary Supervisor Aidan Hopkins
(805) 893-2343
hopkins@ece.ucsb.edu

Secondary Supervisor

Lee Sawyer


Recipes

SignupMonkey: Sign up for this tool


About

This is Karl-Suss model SB-6 substrate bonder. Wafer bonding of pieces to 6” wafers can be done at pressures from 5e-5 to 3e3 mBar and from 50°C to 550°C. This tool mates with the Karl-Suss MA-6 aligner to allow for aligned bonding. Forces up to 20 kN for a 150 mm wafer size are available. The system supports thermal compression as well as anodic bonding (up to 2000 V). The system is computer controlled with a windows environment allowing for multiple recipe steps and saving of recipes and data. The system is configured for manual loading of wafers.

Detailed Specifications

  • Wafer bonding from 50°C to 550°C, +/- 5 degrees accuracy, +/- 3% uniformity
  • Upper and lower heating of samples
  • 5e-5 to 3e3 Torr environment bonding pressure, with Nitrogen
  • Sample size: pieces to 6” wafers, aligned bonding by using the MA/BA-6 aligner - contact supervisor for setup.
  • Anodic bonding to 2000 V
  • Windows-based computer control
  • Wafer bonder currently set up for 4" wafers