E-Beam 1 (Sharon): Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
No edit summary |
→Detailed Specifications: added film limit |
||
| (21 intermediate revisions by 2 users not shown) | |||
| Line 6: | Line 6: | ||
|phone=(805)839-7975 |
|phone=(805)839-7975 |
||
|location=Bay 3 |
|location=Bay 3 |
||
|email= |
|email=mikebarreraz@ece.ucsb.edu |
||
|description = Four Pocket Electron Beam Evaporator |
|description = Four Pocket Electron Beam Evaporator |
||
|manufacturer = Sharon Vacuum Co., Inc. |
|manufacturer = Sharon Vacuum Co., Inc. |
||
|toolid=7 |
|toolid=7 |
||
}} |
}} |
||
[[File:EBEAM1 Controls Sept2022.jpeg|thumb|EBeam#1 Deposition + Beam Controllers]] |
|||
| ⚫ | |||
| ⚫ | |||
The Sharon is a cryo-pumped thin film evaporator with a |
The Sharon is a cryo-pumped thin film evaporator with a Telemark 8 pocket electron beam evaporation source. Fixturing in EBeam1 will accept any size sample up to 4-inch diameter. In addition, a rotation fixture is easily installed which permits adjustable angle, 360° rotation of any size sample, up to 4-inch diameter. This feature is particularly useful for promoting step coverage of irregular surfaces. |
||
| ⚫ | |||
A new fixture allowing up to four - 4" diameter wafers is now installed. |
|||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
*Mechanical Pump: Ebara EV-A10, 35 CFM |
|||
| ⚫ | |||
* |
*Electron Beam Source: Temescal, Model STIH-270-2MB, four 15 cc hearths |
||
*Electron Beam |
*Electron Beam Power Supply: Temescal, Model CV-6SLX, 0 - 10 kV dc, 0–600 mA dc beam current; TemEBeam Sweep Control |
||
| ⚫ | |||
*Electron Beam Power Supply: Temescal, Model CV8A-111, -5 to -10 kV dc, 0.8A dc max. beam current; XYS-8 Sweep Control |
|||
| ⚫ | |||
*Ion Source: Commonwealth Scientific Corp., MOD. 2. Kaufman-type, 3cm ion source; beam currents to 100mA at 1000eV |
|||
*Pieces up to Four - 4" wafers in one run. |
*Pieces up to Four - 4" wafers in one run. |
||
*For single wafers: tilt with motorized rotation and sample lowering for higher effective rates, sidewall coverage, angled evaporation. |
*For single wafers: tilt with motorized rotation and sample lowering for higher effective rates, sidewall coverage, angled evaporation. |
||
*Maximum allowed film thickness: 1µm |
|||
**Please ask supervisor if you need to go thicker |
|||
**Please provide justification for your needs (eg. Not “2 µm is a nice round number”) |
|||
| ⚫ | |||
| ⚫ | |||
**Operating Instructions |
|||
**[https://wiki.nanofab.ucsb.edu/w/images/a/a1/EB1_Rotation_Fixture_SOP_5-16-25.pdf Rotation Fixture SOP] |
|||
**[[E-Beam 1 - 4-inch, 4-wafer Fixture SOP|4-inch, 4-wafer Fixture SOP]] |
|||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
*[[Process Group - Process Control Data#E-Beam 1 (Sharon) - Process Control|'''Process Control Data''']] - Calibration data for the most utilized metals on this sytem. |
|||
| ⚫ | |||
Revision as of 19:36, 22 April 2026
| ||||||||||||||||||||||||||||||

About
The Sharon is a cryo-pumped thin film evaporator with a Telemark 8 pocket electron beam evaporation source. Fixturing in EBeam1 will accept any size sample up to 4-inch diameter. In addition, a rotation fixture is easily installed which permits adjustable angle, 360° rotation of any size sample, up to 4-inch diameter. This feature is particularly useful for promoting step coverage of irregular surfaces.
EBeam1 is used for the evaporation of high purity metals, e.a. Al, Au, Ni, Ge, AuGe, Ti, Pt etc., for interconnect and ohmic contact metallization for fabrication of III-V compound semiconductor and silicon device fabrication.
Detailed Specifications
- Cryopump: CTI Cryotorr 8F with air-cooled compressor
- Pumping speed: 4,000 l/sec. for H2O, 1,500 l/sec. for air, 2,200 l/sec. for H2, 200 l/sec. for Ar
- Mechanical Pump: Ebara EV-A10, 35 CFM
- Electron Beam Source: Temescal, Model STIH-270-2MB, four 15 cc hearths
- Electron Beam Power Supply: Temescal, Model CV-6SLX, 0 - 10 kV dc, 0–600 mA dc beam current; TemEBeam Sweep Control
- Deposition Control: : Inficon IC/5, 6 film programs; 37 parameters for automatic or manual deposition control based on a resonating quartz crystal sensor
- Pieces up to Four - 4" wafers in one run.
- For single wafers: tilt with motorized rotation and sample lowering for higher effective rates, sidewall coverage, angled evaporation.
- Maximum allowed film thickness: 1µm
- Please ask supervisor if you need to go thicker
- Please provide justification for your needs (eg. Not “2 µm is a nice round number”)
Documentation
- EBeam 1 Operating Procedure
- Operating Instructions
- Rotation Fixture SOP
- 4-inch, 4-wafer Fixture SOP
Recipes
- See the E-Beam Recipe Page, for the materials tables and deposition parameters for various materials.
- Process Control Data - Calibration data for the most utilized metals on this sytem.