The NanoFab hosts UCSB Undergraduate Interns throughout the school year and summer. |
The NanoFab hosts UCSB Undergraduate Interns throughout the school year and summer. |
||
No prerequisites/prior knowledge needed; for anyone 16 years old and up; Minimum 6 months commitment (break during summer is acceptable). |
|||
* [[Nanofab Job Postings|Upcoming Internship Openings]] |
|||
* [[Process Group Interns|Current Interns]] |
|||
<br> |
|||
__TOC__ |
|||
=== Internship Goals === |
=== Internship Goals === |
||
Our goals are twofold: |
Our goals are twofold: |
||
# Acquire [[Process Group - Process Control Data|Process Control Data]] so NanoFab staff can proactively identify equipment/process problems, and |
# '''Increased Tool Uptime''': Acquire [[Process Group - Process Control Data|Process Control Data]] so NanoFab staff can proactively identify equipment/process problems, and |
||
# Give [[Process Group Interns|Interns]] hands-on industry-relevant experience to minimize the training required at any microelectronics company/research group. |
# '''Industry-Relevant Experience''': Give [[Process Group Interns|Interns]] hands-on industry-relevant experience to minimize the training required at any microelectronics company/research group. |
||
The skills acquired for each goal are as follows: |
The skills acquired for each goal are as follows: |
||
=== Industry-relevant Experience === |
==== Industry-relevant Experience ==== |
||
| ⚫ | |||
| ⚫ | |||
** Cleanroom safety & protocols such as PPE, safe waste disposal etc. |
** Cleanroom safety & protocols such as PPE, safe waste disposal etc. |
||
** Managing their own schedule to accomplish weekly processing tasks. |
** Managing their own schedule to accomplish weekly processing tasks. |
||
| Line 19: | Line 27: | ||
** Communications with |
** Communications with |
||
*** lab users (scheduling around other users) |
*** lab users (scheduling around other users) |
||
*** equipment |
*** equipment engineers (training, handling/reporting tool issues) |
||
*** process supervisors/managers (reviewing process control data) |
*** process supervisors/managers (reviewing process control data, OCAP actions) |
||
* '''Equipment''': Become comfortable with learning different |
* '''Equipment''': Become comfortable with learning different Operating Procedures of similar tool types |
||
** Eg. 4 different plasma depositions, 4 different ICP etchers etc. |
** Eg. 4 different plasma depositions, 4 different ICP etchers etc. |
||
** Once an intern has learned 3 different PECVD deposition tools, it is trivial to learn a new PECVD tool even from an unfamiliar manufacturer. |
** Once an intern has learned 3 different PECVD deposition tools, it is trivial to learn a new PECVD tool even from an unfamiliar manufacturer. |
||
* [https://en.wikipedia.org/wiki/Manufacturing_execution_system '''MES''']: Learn to utilize production tracking/communications |
* [https://en.wikipedia.org/wiki/Manufacturing_execution_system '''MES''']: Learn to utilize production tracking/communications tools |
||
** Travelers/Process Followers |
** Travelers/Process Followers & associated data directories are created and filled out at run-time for every calibration. (Digital/online via Google Sheets+Drive) |
||
** |
** Combining ''Equipment Operating Procedures'' with ''Process Travelers'' instructions at run-time. |
||
** Data collection with standardized digital filenames |
** Data collection with standardized digital filenames & directory structures, available online to all lab users. |
||
** [https://docs.google.com/spreadsheets/d/1fTDNXxpf4tgNYLIEs_jvehG1KvtXqqTRDBI7sHNAVvo/edit?gid=0#gid=0 Click on the '''date''' of any SPC data row here to see a Traveler & Data folder] filled out by interns (or here is [https://drive.google.com/drive/folders/10v4pElyxNBTe4kJw8fMtuBtj54M5vkPx one example]). |
|||
*** Every Calibration process has the same format: see other intern-run processes here: [[Process Group - Process Control Data|Process Control Data]] |
|||
* '''[https://en.wikipedia.org/wiki/Statistical_process_control SPC]''': Perform metrology, process control, create SPC charts |
* '''[https://en.wikipedia.org/wiki/Statistical_process_control SPC]''': Perform metrology, process control, create SPC charts |
||
** Data from the Travelers are entered into online spreadsheets, which calculate SPC charts |
** Data from the Travelers are entered into online spreadsheets, which calculate SPC charts |
||
** Some interns create/modify SPC charts when needed for newly developed Cals. |
** Some interns create/modify SPC charts when needed for newly developed Cals. |
||
** See the intern-generated SPC data here: [[Process Group - Process Control Data|Process Control Data]] |
|||
* '''OCAP/Repair''': Work with tool engineers to identify & diagnose equipment problems. |
* '''OCAP/Repair''': Work with tool engineers to identify & diagnose equipment problems. |
||
** If Process Engineers identify an Out-of-Control process, Interns are involved in the communications & testing of tool repairs. |
** If Process Engineers identify an Out-of-Control process, Interns are involved in the communications & testing of tool repairs, until process is back "in control". |
||
=== Process Control for Increased Uptime === |
==== Process Control (SPC) for Increased Uptime ==== |
||
| ⚫ | |||
| ⚫ | |||
* Calibration processes are identical each time (unlike lab user's processes), allowing apples-to-apples comparisons. |
* Calibration processes are identical each time (unlike lab user's processes), allowing apples-to-apples comparisons. |
||
* Regular meetings with Process Engineers allow us to proactively identify equipment/process issues, failing tool components, and schedule repairs/remedies sooner than if detected by a lab user. |
* Regular meetings with Process Engineers allow us to proactively identify equipment/process issues, failing tool components, and schedule repairs/remedies sooner than if detected by a lab user. |
||
| Line 50: | Line 60: | ||
=== Phase 1: Deposition Cals (1st Quarter) === |
=== Phase 1: Deposition Cals (1st Quarter) === |
||
* Interns |
* Interns run 4 different deposition tools weekly, in the following order: |
||
** Plasmatherm PECVD 1 |
** [[PECVD 1 (PlasmaTherm 790)|Plasmatherm PECVD 1]] |
||
** Advanced Vacuum PECVD 2, |
** [[PECVD 2 (Advanced Vacuum)|Advanced Vacuum PECVD 2]], |
||
** Unaxis ICP-PECVD, |
** [[ICP-PECVD (Unaxis VLR)|Unaxis ICP-PECVD]], |
||
** Veeco Ion Beam Deposition |
** [[Ion Beam Deposition (Veeco NEXUS)|Veeco Ion Beam Sputter Deposition]] |
||
** 3-4 different films (SiO<sub>2</sub>, Si<sub>3</sub>N<sub>4</sub>, Low-stress-Si<sub>3</sub>N<sub>4</sub>) are run on <u>each tool</u>. |
** 3-4 different films (SiO<sub>2</sub>, Si<sub>3</sub>N<sub>4</sub>, Low-stress-Si<sub>3</sub>N<sub>4</sub>) are run on <u>each tool</u>. |
||
* Every film undergoes the following metrology: |
* Every film undergoes the following metrology: |
||
** Ellipsometry: Thin-film thickness and refractive index at 2 different wavelengths. |
** [[Ellipsometer (Woollam)|Ellipsometry]]: Thin-film thickness and refractive index at 2 different wavelengths. |
||
** Reflectometry Wafer Mapping: Thin-film Uniformity across the wafer. |
** [[Optical Film Thickness & Wafer-Mapping (Filmetrics F50)|Reflectometry Wafer Mapping]]: Thin-film Uniformity across the wafer. |
||
** Particle Count: laser-scanning via Surfscan, at two different particle-size/range settings |
** [[Surface Analysis (KLA/Tencor Surfscan)|Particle Count]]: laser-scanning via Surfscan, at two different particle-size/range settings |
||
** Thin-Film Stress: requires before & after wafer bow measurements via laser scanning |
** [[Film Stress (Tencor Flexus)|Thin-Film Stress]]: requires before & after wafer bow measurements via laser scanning |
||
* Follow Process Protocols: |
|||
** Follow and Record Data onto Travelers for every Cal run, save metro data into publicly-accessible folders. |
|||
** Update all [[Process Group - Process Control Data|SPC data tables]] and charts accurately, report any "out of control" process issues. |
|||
* By the end of 1st Quarter, Interns are running 9-12 thin-film cals every 2 weeks. |
* By the end of 1st Quarter, Interns are running 9-12 thin-film cals every 2 weeks. |
||
=== Phase 2: EtchCals and LithoCals (2nd Quarter) === |
=== Phase 2: EtchCals and LithoCals (2nd Quarter) === |
||
* Interns |
* Interns run 4 different ICP Etchers weekly: |
||
** Plasmatherm SLR Fluorine Etcher |
** [[Fluorine ICP Etcher (PlasmaTherm/SLR Fluorine ICP)|Plasmatherm SLR Fluorine ICP Etcher]] - SiO2 and Si etching |
||
** Oxford Cobra III-V Etcher |
** [[Oxford ICP Etcher (PlasmaPro 100 Cobra)|Oxford Cobra III-V ICP Etcher]] - InP etching |
||
** Plasmatherm DSEiii |
** [[DSEIII (PlasmaTherm/Deep Silicon Etcher)|Plasmatherm DSEiii]] - Bosch etching of Silicon |
||
** Panasonic ICP #2 |
** [[ICP Etch 2 (Panasonic E626I)|Panasonic ICP #2]] - SiO2 and GaAs etching |
||
** 1-2 different Etches per tool; one "insensitive" to chamber condition, one "sensitive" to chamber condition. |
** 1-2 different Etches per tool; one "insensitive" to chamber condition, one "sensitive" to chamber condition. |
||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
* Metrology on each EtchCal: |
* Metrology on each EtchCal: |
||
** SEM of manually Cleaved Cross-section |
** [[SEM 1 (JEOL IT800SHL)|SEM]] of manually Cleaved Cross-section |
||
** Cleaving samples for cross-sectional SEM. |
|||
** Profilometry & Etch-Rate Calculation |
** [[Step Profilometer (DektakXT)|Profilometry]] & Etch-Rate Calculation |
||
** Etch Selectivity Calculation via pre/post hardmask removal profilometry |
** Etch Selectivity Calculation via pre/post hardmask removal profilometry |
||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
* Metro on each LithoCal: |
* Metro on each LithoCal: |
||
** SEM for Critical Dimension measurement; multiple locations on wafer. |
** [[SEM 1 (JEOL IT800SHL)|SEM]] for Critical Dimension measurement; multiple locations on wafer. |
||
** Identification of "hotspot" particulate contamination on wafer/tool. |
** Identification of "hotspot" particulate contamination on wafer/tool. |
||
* Follow Process Protocols: |
|||
| ⚫ | |||
** Follow and Record Data onto Travelers for every Cal run, save metro data into publicly-accessible folders. |
|||
** Update all [[Process Group - Process Control Data|SPC data tables]] and charts accurately, report any "out of control" process issues. |
|||
| ⚫ | |||
Latest revision as of 00:33, 11 January 2026
The NanoFab hosts UCSB Undergraduate Interns throughout the school year and summer.
No prerequisites/prior knowledge needed; for anyone 16 years old and up; Minimum 6 months commitment (break during summer is acceptable).
Internship Goals
Our goals are twofold:
- Increased Tool Uptime: Acquire Process Control Data so NanoFab staff can proactively identify equipment/process problems, and
- Industry-Relevant Experience: Give Interns hands-on industry-relevant experience to minimize the training required at any microelectronics company/research group.
The skills acquired for each goal are as follows:
Industry-relevant Experience
- Protocols: Interns become comfortable in a busy semiconductor 'fab environment. After 2-3 months of regular usage the interns are fully comfortable with:
- Cleanroom safety & protocols such as PPE, safe waste disposal etc.
- Managing their own schedule to accomplish weekly processing tasks.
- Multi-tasking to run simultaneous processes fast and efficiently.
- Interns learn new tools only once their current cals have been condensed into a few hours.
- Communications with
- lab users (scheduling around other users)
- equipment engineers (training, handling/reporting tool issues)
- process supervisors/managers (reviewing process control data, OCAP actions)
- Equipment: Become comfortable with learning different Operating Procedures of similar tool types
- Eg. 4 different plasma depositions, 4 different ICP etchers etc.
- Once an intern has learned 3 different PECVD deposition tools, it is trivial to learn a new PECVD tool even from an unfamiliar manufacturer.
- MES: Learn to utilize production tracking/communications tools
- Travelers/Process Followers & associated data directories are created and filled out at run-time for every calibration. (Digital/online via Google Sheets+Drive)
- Combining Equipment Operating Procedures with Process Travelers instructions at run-time.
- Data collection with standardized digital filenames & directory structures, available online to all lab users.
- Click on the date of any SPC data row here to see a Traveler & Data folder filled out by interns (or here is one example).
- Every Calibration process has the same format: see other intern-run processes here: Process Control Data
- SPC: Perform metrology, process control, create SPC charts
- Data from the Travelers are entered into online spreadsheets, which calculate SPC charts
- Some interns create/modify SPC charts when needed for newly developed Cals.
- See the intern-generated SPC data here: Process Control Data
- OCAP/Repair: Work with tool engineers to identify & diagnose equipment problems.
- If Process Engineers identify an Out-of-Control process, Interns are involved in the communications & testing of tool repairs, until process is back "in control".
Process Control (SPC) for Increased Uptime
- Interns run process-control on the lab's most critical/high-usage tools & update SPC charts.
- Calibration processes are identical each time (unlike lab user's processes), allowing apples-to-apples comparisons.
- Regular meetings with Process Engineers allow us to proactively identify equipment/process issues, failing tool components, and schedule repairs/remedies sooner than if detected by a lab user.
- Lab users are notified of process anomalies & repair plans, reducing bad outcomes for lab users.
- "Contamination" checks via On-Demand process-checks
- Determine whether a new process affects other processes on the same tool, by running pre/post Cal Etches.
- On ICP Etchers, enables data-driven equipment sharing between processes.
- Enables lab-users to quickly determine whether problems lie with the Equipment/"contamination", another user's process or their own Process.
Job Description: 2 phases
Internships are generally run in 2 phases, with each phase being approx. 1 Quarter (3 months) long.
Phase 1: Deposition Cals (1st Quarter)
- Interns run 4 different deposition tools weekly, in the following order:
- Plasmatherm PECVD 1
- Advanced Vacuum PECVD 2,
- Unaxis ICP-PECVD,
- Veeco Ion Beam Sputter Deposition
- 3-4 different films (SiO2, Si3N4, Low-stress-Si3N4) are run on each tool.
- Every film undergoes the following metrology:
- Ellipsometry: Thin-film thickness and refractive index at 2 different wavelengths.
- Reflectometry Wafer Mapping: Thin-film Uniformity across the wafer.
- Particle Count: laser-scanning via Surfscan, at two different particle-size/range settings
- Thin-Film Stress: requires before & after wafer bow measurements via laser scanning
- Follow Process Protocols:
- Follow and Record Data onto Travelers for every Cal run, save metro data into publicly-accessible folders.
- Update all SPC data tables and charts accurately, report any "out of control" process issues.
- By the end of 1st Quarter, Interns are running 9-12 thin-film cals every 2 weeks.
Phase 2: EtchCals and LithoCals (2nd Quarter)
- Interns run 4 different ICP Etchers weekly:
- Plasmatherm SLR Fluorine ICP Etcher - SiO2 and Si etching
- Oxford Cobra III-V ICP Etcher - InP etching
- Plasmatherm DSEiii - Bosch etching of Silicon
- Panasonic ICP #2 - SiO2 and GaAs etching
- 1-2 different Etches per tool; one "insensitive" to chamber condition, one "sensitive" to chamber condition.
- Metrology on each EtchCal:
- SEM of manually Cleaved Cross-section
- Cleaving samples for cross-sectional SEM.
- Profilometry & Etch-Rate Calculation
- Etch Selectivity Calculation via pre/post hardmask removal profilometry
- Interns run weekly ASML DUV Stepper lithography: photoresist coating, exposure and develop.
- Critical particulate-sensitive process, cal shows any particles present
- Intern's techniques are remedied if particles are detected.
- Critical particulate-sensitive process, cal shows any particles present
- Metro on each LithoCal:
- SEM for Critical Dimension measurement; multiple locations on wafer.
- Identification of "hotspot" particulate contamination on wafer/tool.
- Follow Process Protocols:
- Follow and Record Data onto Travelers for every Cal run, save metro data into publicly-accessible folders.
- Update all SPC data tables and charts accurately, report any "out of control" process issues.
- By the end of 2nd Quarter, Interns are running LithoCals and ~2 EtchCals weekly, with multiple SEM sessions. They are proficient at SEM by the end of the 2nd quarter.